Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 54 - 66 g/10 min @Load 2.16 kg, Temperature 190 °C |
54 - 66 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4026Z (26460) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 54 - 66 g/10 min @Load 21.6 kg, Temperature 190 °C |
54 - 66 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4116P (16402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 54 - 66 g/10 min @Load 21.6 kg, Temperature 190 °C |
54 - 66 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4118N (18401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 54 - 66 g/10 min @Load 21.6 kg, Temperature 190 °C |
54 - 66 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 5117P (18602) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 54 - 66 g/10 min @Load 21.6 kg, Temperature 190 °C |
54 - 66 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 5118P (18602) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 54 - 66 g/10 min @Load 21.6 kg, Temperature 190 °C |
54 - 66 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4115P (16402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 54 - 66 g/10 min @Load 21.6 kg, Temperature 190 °C |
54 - 66 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4117P (18402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 54 - 66 g/10 min @Load 21.6 kg, Temperature 190 °C |
54 - 66 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4118P (18402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |