Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 65 g/10 min @Load 5.00 kg, Temperature 200 °C |
65 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G6713-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G6713-0001 is an easy processing TPE designed for use in injection molding and extrusion applications where an extremely soft feel is desired. - Excellent Colorability - Good Ozone and UV.. |
|||
Melt Flow | 65 g/10 min @Load 10.0 kg, Temperature 220 °C |
65 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Kingfa HF-606 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmHigh flowModerate UV stabilityHigh stiffnessApplications:Injection moldingMonitor cabinetCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co.,.. |
|||
Melt Flow | 65 g/10 min @Load 10.0 kg, Temperature 220 °C |
65 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical HIPS 60HRI PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: TV Sets, Tape Recorders, Vacuum Cleaner, Washing Machine, Air ConditionerCAS: 9003-55-8Information provided by LG Che.. |
|||
Melt Flow | 65 g/10 min @Load 5.00 kg, Temperature 200 °C |
65 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133H |
Total Lacqrene® 740 High Impact Polystyrene
(discontinued **) LACQRENE® alpha 740 is a high gloss, high impact grade of polystyrene.ApplicationWhite goods (washing machines, driers), Toys and games, Garden equipment, All applications needing high gloss with g.. |