Physical Properties Metric English Comments
Melt Flow 54 - 66 g/10 min

@Load 2.16 kg,
Temperature 190 °C
54 - 66 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4026Z (26460) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 54 - 66 g/10 min

@Load 21.6 kg,
Temperature 190 °C
54 - 66 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 4116P (16402) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 54 - 66 g/10 min

@Load 21.6 kg,
Temperature 190 °C
54 - 66 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 4118N (18401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 54 - 66 g/10 min

@Load 21.6 kg,
Temperature 190 °C
54 - 66 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 5117P (18602) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 54 - 66 g/10 min

@Load 21.6 kg,
Temperature 190 °C
54 - 66 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 5118P (18602) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 54 - 66 g/10 min

@Load 21.6 kg,
Temperature 190 °C
54 - 66 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 4115P (16402) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 54 - 66 g/10 min

@Load 21.6 kg,
Temperature 190 °C
54 - 66 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 4117P (18402) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 54 - 66 g/10 min

@Load 21.6 kg,
Temperature 190 °C
54 - 66 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 4118P (18402) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer