Polymer Property : Oxygen Transmission Rate = 54.2 cc/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission Rate 841 cc/m²/day

@Pressure 0.101 MPa,
Temperature 30.0 °C
54.2 cc/100 in²/day

@Pressure 14.7 psi,
Temperature 86.0 °F
ASTM D1434
Eastman Eastman AP005 Copolyester
Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly..