Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 1.10 cc/m²/day | 0.0708 cc/100 in²/day | 77°F / 0% / RH; ASTM D3985 |
Honeywell Capran® Emblem™ MT1500 Bi-Axially Oriented Nylon 6 Film Description: Capran® Emblem™ MT1500 is a 0.60 mil (15 micron) biaxially oriented nylon 6 film with a metallized barrier coating well suited for high barrier packaging applications. Informati.. |
|||
Oxygen Transmission Rate | 1.10 cc/m²/day | 0.0708 cc/100 in²/day | 77°F / 0% / RH; ASTM D3985 |
Honeywell Capran® Emblem™ MT2500 Bi-Axially Oriented Nylon 6 Film Description: Capran® Emblem™ MT2500 is a 1.00 mil (25 micron) biaxially oriented nylon 6 film with a metallized barrier coating.Applications: Capron® Emblem™ MT2500 is well suited fo.. |