Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 40.0 - 1000 cc/m²/day | 2.58 - 64.4 cc/100 in²/day | Average value: 292 cc/m²/day Grade Count:6 |
Overview of materials for Polyvinyl Dichloride (PVDC) This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap.. |