Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 132 g/m²/day | 8.50 g/100 in²/day | ASTM F372 |
Eastman Eastman AP005 Copolyester Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly.. |