Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 40.0 g/m²/day | 2.58 g/100 in²/day | 0.1 mm thick disc |
Lucite International Colacryl ® TS1173 Reactive Acrylic Syrup Lucite® Colacryl® TS1173 is a reactive polymer solution containing dissolved polymers, plasticiser and a polymerisation activator.Information provided by Lucite International |
|||
Water Vapor Transmission | 40.0 g/m²/day | 2.58 g/100 in²/day | ASTM E96 Procedure E |
DuPont Teijin Films Mylar® HS Polyester Film, 65 Gauge (17 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester packaging film designed for heat shrink applications. It is currently available in 48, 65, 80, and 150 gauges, and othe.. |