Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 11.0 g/m²/day @Thickness 0.00100 mm, Temperature 38.0 °C |
0.708 g/100 in²/day @Thickness 0.0000394 in, Temperature 100 °F |
90% RH; ASTM F1249 |
Solvay Specialty Polymers Diofan® B 203 Polyvinylidene Chloride (PVDC) Diofan® B 203 is a PVDC latex with outstanding impermeability to gases and moisture. It is particularly recommended for coatings on plastic films.Features: Moisture Barrier; Oxygen BarrierUses: B.. |
|||
Water Vapor Transmission | 11.0 g/m²/day @Thickness 0.00100 mm, Temperature 38.0 °C |
0.708 g/100 in²/day @Thickness 0.0000394 in, Temperature 100 °F |
90% RH; ASTM F1249 |
Solvay Specialty Polymers Diofan® B 204 Polyvinylidene Chloride (PVDC) Diofan® B 204 is a PVDC latex with outstanding impermeability to gases and moisture. It is particularly recommended for coatings on plastic films.Uses: Coating ApplicationsAdditional Properties: .. |
|||
Water Vapor Transmission | 11.0 g/m²/day @Temperature 37.8 °C |
0.708 g/100 in²/day @Temperature 100 °F |
90% RH; thickness not specified; ASTM E96 |
Total PPH 3571 Polypropylene, Film Extrusion Grade Homopolymer film gradeLow Residuals - Fina 3571 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock - Fina.. |
|||
Water Vapor Transmission | 11.0 g/m²/day @Temperature 37.8 °C |
0.708 g/100 in²/day @Temperature 100 °F |
90% RH; thickness not specified; ASTM E96 |
Total PPR 6573XHC Polypropylene, Random Copolymer Film Grade Random copolymer film gradeColor - Low catalyst residuals in FINA 6573XHC result in improved color stability.Clarity/Impact - The random copolymer structure of FINA 6573XHC improves its clarity and .. |
|||
Water Vapor Transmission | 11.0 g/m²/day @Temperature 37.8 °C |
0.708 g/100 in²/day @Temperature 100 °F |
90% RH; thickness not specified; ASTM E96 |
Total PPR 7450HC Polypropylene, Film Extrusion Grade Random copolymer heat sealable film gradeColor - Low catalyst residuals in FINA 7450HC result in improved color stability.Clarity/Impact - The random copolymer structure of FINA 7450HC improves its .. |
|||
Water Vapor Transmission | 11.0 - 160 g/m²/day @Temperature 38.0 - 38.0 °C |
0.708 - 10.3 g/100 in²/day @Temperature 100 - 100 °F |
Average value: 50.7 g/m²/day Grade Count:9 |
Overview of materials for Polyvinyl Dichloride (PVDC) This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap.. |
|||
Water Vapor Transmission | 11.0 - 160 g/m²/day @Thickness 0.00100 - 0.00100 mm |
0.708 - 10.3 g/100 in²/day @Thickness 0.0000394 - 0.0000394 in |
Average value: 50.7 g/m²/day Grade Count:9 |
Overview of materials for Polyvinyl Dichloride (PVDC) This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap.. |