Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 2.60 g/m²/day | 0.167 g/100 in²/day | 100°F / 100%RH); ASTM F1249 |
Honeywell Capran® Emblem™ MT1500 Bi-Axially Oriented Nylon 6 Film Description: Capran® Emblem™ MT1500 is a 0.60 mil (15 micron) biaxially oriented nylon 6 film with a metallized barrier coating well suited for high barrier packaging applications. Informati.. |
|||
Water Vapor Transmission | 2.60 g/m²/day | 0.167 g/100 in²/day | 100°F / 100%RH); ASTM F1249 |
Honeywell Capran® Emblem™ MT2500 Bi-Axially Oriented Nylon 6 Film Description: Capran® Emblem™ MT2500 is a 1.00 mil (25 micron) biaxially oriented nylon 6 film with a metallized barrier coating.Applications: Capron® Emblem™ MT2500 is well suited fo.. |
|||
Water Vapor Transmission | 2.60 g/m²/day | 0.167 g/100 in²/day | 38°C, 90% RH; ExxonMobil Method |
ExxonMobil Bicor® 210 ASB-X OPP Film Product Description: Bicor ASB-X is a two side coated, sealable OPP film designed for broad use in many applications, including overwrap, horizontal, and vertical packaging. This film is suitable as.. |
|||
Water Vapor Transmission | 2.60 - 465 g/m²/day | 0.167 - 29.9 g/100 in²/day | Average value: 143 g/m²/day Grade Count:19 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |