Polymer Property : Water Vapor Transmission = 40.0 g/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 40.0 g/m²/day
2.58 g/100 in²/day
0.1 mm thick disc
Lucite International Colacryl ® TS1173 Reactive Acrylic Syrup
Lucite® Colacryl® TS1173 is a reactive polymer solution containing dissolved polymers, plasticiser and a polymerisation activator.Information provided by Lucite International
Water Vapor Transmission 40.0 g/m²/day
2.58 g/100 in²/day
ASTM E96 Procedure E
DuPont Teijin Films Mylar® HS Polyester Film, 65 Gauge (17 µm)
Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester packaging film designed for heat shrink applications. It is currently available in 48, 65, 80, and 150 gauges, and othe..