Polymer Property : Water Vapor Transmission = 11.0 g/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 11.0 g/m²/day

@Thickness 0.00100 mm,
Temperature 38.0 °C
0.708 g/100 in²/day

@Thickness 0.0000394 in,
Temperature 100 °F
90% RH; ASTM F1249
Solvay Specialty Polymers Diofan® B 203 Polyvinylidene Chloride (PVDC)
Diofan® B 203 is a PVDC latex with outstanding impermeability to gases and moisture. It is particularly recommended for coatings on plastic films.Features: Moisture Barrier; Oxygen BarrierUses: B..
Water Vapor Transmission 11.0 g/m²/day

@Thickness 0.00100 mm,
Temperature 38.0 °C
0.708 g/100 in²/day

@Thickness 0.0000394 in,
Temperature 100 °F
90% RH; ASTM F1249
Solvay Specialty Polymers Diofan® B 204 Polyvinylidene Chloride (PVDC)
Diofan® B 204 is a PVDC latex with outstanding impermeability to gases and moisture. It is particularly recommended for coatings on plastic films.Uses: Coating ApplicationsAdditional Properties: ..
Water Vapor Transmission 11.0 g/m²/day

@Temperature 37.8 °C
0.708 g/100 in²/day

@Temperature 100 °F
90% RH; thickness not specified; ASTM E96
Total PPH 3571 Polypropylene, Film Extrusion Grade
Homopolymer film gradeLow Residuals - Fina 3571 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock - Fina..
Water Vapor Transmission 11.0 g/m²/day

@Temperature 37.8 °C
0.708 g/100 in²/day

@Temperature 100 °F
90% RH; thickness not specified; ASTM E96
Total PPR 6573XHC Polypropylene, Random Copolymer Film Grade
Random copolymer film gradeColor - Low catalyst residuals in FINA 6573XHC result in improved color stability.Clarity/Impact - The random copolymer structure of FINA 6573XHC improves its clarity and ..
Water Vapor Transmission 11.0 g/m²/day

@Temperature 37.8 °C
0.708 g/100 in²/day

@Temperature 100 °F
90% RH; thickness not specified; ASTM E96
Total PPR 7450HC Polypropylene, Film Extrusion Grade
Random copolymer heat sealable film gradeColor - Low catalyst residuals in FINA 7450HC result in improved color stability.Clarity/Impact - The random copolymer structure of FINA 7450HC improves its ..
Water Vapor Transmission 11.0 - 160 g/m²/day

@Temperature 38.0 - 38.0 °C
0.708 - 10.3 g/100 in²/day

@Temperature 100 - 100 °F
Average value: 50.7 g/m²/day Grade Count:9
Overview of materials for Polyvinyl Dichloride (PVDC)
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap..
Water Vapor Transmission 11.0 - 160 g/m²/day

@Thickness 0.00100 - 0.00100 mm
0.708 - 10.3 g/100 in²/day

@Thickness 0.0000394 - 0.0000394 in
Average value: 50.7 g/m²/day Grade Count:9
Overview of materials for Polyvinyl Dichloride (PVDC)
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap..