Physical Properties Metric English Comments
Water Vapor Transmission 104 g/m²/day
6.70 g/100 in²/day
JIS Z0208
DuPont Teijin Films Teonex® Q51 Polyester Film, 48 Gauge
Teonex® Q51 is biaxially oriented polyethylene naphthalate (PEN) film. It is slightly hazy with excellent handling properties for general purpose. It is commercially available in nominal 48 - 1000 ..