Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Vapor Pressure = 0.000267 bar Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Vapor Pressure 0.000267 bar

@Temperature 170 °C
0.200 torr

@Temperature 338 °F
LG Chemical BPA
Structure & Characteristics: (CH3)2C(C6H4OH)2 . BPA is an us powder with white colorOverview: Bisphenol-A(BPA) is used primarily to make polycarbonate and epoxy resins, both of which are used in a w..
Vapor Pressure 0.000267 bar

@Temperature 20.0 °C
0.200 torr

@Temperature 68.0 °F
LyondellBasell Glycol Ether DM Diethylene glycol methyl ether
Information provided by Lyondell.
Vapor Pressure 0.000267 bar

@Temperature 25.0 °C
0.200 torr

@Temperature 77.0 °F
Solvay Specialty Polymers Galden® HT200 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..
Vapor Pressure 0.000267 bar

@Temperature 150 °C
0.200 torr

@Temperature 302 °F
ASTM D2879
ExxonMobil SpectraSyn Plus™ 3.6 Advanced Polyalphaolefin (PAO) Fluid
Product Description: SpectraSyn Plus™ Advanced Polyalphaolefin (PAO) provide an optimal combination of volatility and low-temperature fluidity. SpectraSyn Plus™ Advanced products viscosity indices..
Vapor Pressure 0.000267 bar

@Temperature 150 °C
0.200 torr

@Temperature 302 °F
ASTM D2879
ExxonMobil SpectraSyn Plus™ 4 Advanced Polyalphaolefin (PAO) Fluid
Product Description: SpectraSyn Plus™ Advanced Polyalphaolefin (PAO) provide an optimal combination of volatility and low-temperature fluidity. SpectraSyn Plus™ Advanced products viscosity indices..
Vapor Pressure 0.000267 bar

@Temperature 150 °C
0.200 torr

@Temperature 302 °F
ASTM D2879
ExxonMobil SpectraSyn™ 4 Polyalphaolefin (PAO) Fluid
Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) ..
Vapor Pressure 0.000267 bar

@Temperature 150 °C
0.200 torr

@Temperature 302 °F
ASTM D2879
ExxonMobil SpectraSyn Plus™ 6 Advanced Polyalphaolefin (PAO) Fluid
Product Description: SpectraSyn Plus™ Advanced Polyalphaolefin (PAO) provide an optimal combination of volatility and low-temperature fluidity. SpectraSyn Plus™ Advanced products viscosity indices..
Vapor Pressure 0.000267 bar

@Temperature 20.0 °C
0.200 torr

@Temperature 68.0 °F
ExxonMobil Method
ExxonMobil Varsol™ 80 Non-dearomatized Fluid
Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East and EuropeInformation provided by ExxonMobil
Vapor Pressure 0.000267 bar
0.200 torr
Abatron ClearStrip™ Stripper for Paint, Varnish, Coatings; Gel
ClearStrip™ is a high-performance gel designed to remove multiple coats of paint safely. It wets the paint surface for a long time, which allows the paint loosening process to continue for longer t..
Vapor Pressure 0.000267 bar
0.200 torr
3M CC-2 Cable Cleaning Preparation Kits
3M CC series Cable Cleaning Solvent is a full strength non-ozone depleting solvent cleaner, degreaser for use as an effective replacement for 1,1,1-Trichloroethane and other hazardous solvents, Form..
Vapor Pressure 0.000267 bar
0.200 torr
3M CC-3 Cleaning Pad Kits
3M CC series Cable Cleaning Solvent is a full strength non-ozone depleting solvent cleaner, degreaser for use as an effective replacement for 1,1,1-Trichloroethane and other hazardous solvents, Form..
Vapor Pressure 0.000267 bar
0.200 torr
3M CC-4 Cleaning Solvent
3M CC series Cable Cleaning Solvent is a full strength non-ozone depleting solvent cleaner, degreaser for use as an effective replacement for 1,1,1-Trichloroethane and other hazardous solvents, Form..
Copyright © lookpolymers.com All Rights Reserved