Physical Properties Metric English Comments
Thickness 191 - 241 microns
7.50 - 9.50 mil
Overall
Arlon 5163X0085 0.0085" (0.216 mm) Cured Silicone Rubber with Fiberglass Substrate  (discontinued **)
50 inches Overall Width. Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone RubberProduct Description: Acoustical dampeningAppearance: Silver silicone on fiberglass clothThis d..
Thickness 203 - 241 microns
8.00 - 9.50 mil
Overall
Arlon 44571B008 0.0085" (0.216 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place ..
Thickness 203 - 241 microns
8.00 - 9.50 mil
Overall
Arlon 44571R008A 0.0085" (0.216 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place ..
Thickness 203 - 241 microns
8.00 - 9.50 mil
Overall
Arlon 44576B009A 0.0085" (0.216 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place of..
Thickness 216 - 241 microns
8.50 - 9.50 mil
Adhesive and protective top covering
3M 3635-100 Light Enhancement Film
A light box or channel letter contains lighting elements that illuminate the front sign face and transmit some light to the viewer. However much of the illumination is reflected or absorbed by other..
Copyright © lookpolymers.com All Rights Reserved