Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-11 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-196 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-197 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-25 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-47 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-63 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-77 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-15 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-186 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-187 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-193 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-25 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-56 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-64 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-98 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-139 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-307 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-31 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-49 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-53 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-177 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-263 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-31 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-38 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-41 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-46 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-48 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-59 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-86 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-99 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |