Physical Properties Metric English Comments
Thickness 25.0 - 80.0 microns
0.984 - 3.15 mil
Recommended
Polimeri Europa Riblene® FL 20 Low Density Polyethylene - Blown Film Extrusion
Riblene FL 20 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FL 20 is characterized by a good balance between processability and mechanical properties.Films manufac..
Thickness 25.0 - 80.0 microns
0.984 - 3.15 mil
Recommended
Polimeri Europa Riblene® FL 23 Low Density Polyethylene - Blown Film Extrusion
Riblene FL 23 is a low density polyethylene (LDPE) with added slip agent, suitable for blown film extrusion. Riblene FL 23 is characterized by a good balance between processability and mechanical p..
Thickness 25.0 - 80.0 microns
0.984 - 3.15 mil
Recommended
Polimeri Europa Riblene® FL 24 Low Density Polyethylene - Blown Film Extrusion
Riblene FL 24 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 24 is characterized by a good balance between processabilit..
Thickness 25.0 - 80.0 microns
0.984 - 3.15 mil
Recommended
Polimeri Europa Riblene® FL 30 Low Density Polyethylene - Blown Film Extrusion
Riblene FL 30 is a low density polyethylene (LDPE) ideal for blown film extrusion. Riblene FL 30 is characterized by a good balance between processability, mechanical and optical properties.Films m..
Thickness 25.0 - 80.0 microns
0.984 - 3.15 mil
Recommended
Polimeri Europa Riblene® FL 34 E Low Density Polyethylene - Blown Film Extrusion
Riblene FL 34 E is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 34 E is characterized by a good balance between processab..
Thickness 25.0 - 80.0 microns
0.984 - 3.15 mil
Recommended
Polimeri Europa Riblene® FL 34 Low Density Polyethylene - Blown Film Extrusion
Riblene FL 34 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 34 is characterized by a good balance between processabilit..
Thickness 40.0 - 80.0 microns
1.57 - 3.15 mil
Möller Medical PolySkin 98 S NanoCoating
Flexible, non-abrasive "soft feel" coating with velour-like surface.Information provided by Möller Medical, Member of CENTROTEC Group
Thickness 40.0 - 80.0 microns
1.57 - 3.15 mil
Indium Corp. NanoFoil® NF40 Nickel and Aluminum Localized Heat Source For Bonding
Features:40 microns thick - optimized for bonding electronics assembliesMinimum dimension 1.2mm x 2.0mmLocalized heat source for bondingEnables high-strength, high conductivity bonds between most co..
Thickness 30.0 - 80.0 microns
1.18 - 3.15 mil
Daikin NEOFLON ACX-31 PFA Coating Powder, White
NEOFLON PFA coating powder is designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 30-80 micron thickness.Processing Methods: Electrostati..
Thickness 30.0 - 80.0 microns
1.18 - 3.15 mil
Daikin NEOFLON ACX-34 PFA Coating Powder, White
NEOFLON PFA coating powder is designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 30-80 micron thickness.Processing Methods: Electrostati..
Thickness 70.0 - 80.0 microns
2.76 - 3.15 mil
CEN® Electronic Material CN Polyimide Film, 3 Mil Thickness
CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca..
Thickness 70.0 - 80.0 microns
2.76 - 3.15 mil
ASTM D374
CEN® Electronic Material CV Polyimide Film, 3 Mil Thickness
CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup..