Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Side 1 |
Arlon 10502R010 0.010" (.254 mm) Cured/Post-Cured Unsupported Silicone Rubber Design/Construction:Side 1: Cured/Post-Cured Unsupported Silicone RubberAppearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used to.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Overall |
Arlon 10502R010 0.010" (.254 mm) Cured/Post-Cured Unsupported Silicone Rubber Design/Construction:Side 1: Cured/Post-Cured Unsupported Silicone RubberAppearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used to.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Overall |
Arlon 30540R010 0.010" (0.254 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier This data represents typical values for the production material. The data should not be used to write, or in plac.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Side 1 |
Arlon 30540R010 0.010" (0.254 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier This data represents typical values for the production material. The data should not be used to write, or in plac.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Overall |
Arlon 30570R010 0.010" (0.254 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Side 1 |
Arlon 30570R010 0.010" (0.254 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The.. |
|||
Thickness | 240 - 280 microns | 9.45 - 11.0 mil | |
AK Steel TRAN-COR® H-1 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Thickness | 240 - 280 microns | 9.45 - 11.0 mil | |
AK Steel TRAN-COR® H-1 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Overall |
Arlon 30580R010 0.010" (0.254 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Side 1 |
Arlon 30580R010 0.010" (0.254 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Overall |
Arlon 44571R010A 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Overall |
Arlon 44572R010 0.010" (0.254 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberAppearance: Red silicone rubber on fiberglass clothThis data represents typical values for the production material. The data should not be used to wr.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | film and adhesive |
3M 7000PL Photoluminescent Film 3M Photoluminscent Film 7000PL is a high performance photoluminescent for film for safety and emergency exit signage. Meets and exceeds ASTM E207210, IMO A.752, OSHA 1910, 2000 IBC, DIN-67510 Part 4.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 49090R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass fabricThis data Represents typical values for the production material. The data should not be used to wr.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Overall |
Arlon 44250R011 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be used to wri.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Overall |
Arlon 44560R009W 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Appearance Red silicone gum on glass fabricThis data represents typical values for the production material. The data should not be used to write, .. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Overall |
Arlon 44560R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not be used to w.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Overall |
Arlon 44570B010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Layers Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place of, material specificati.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Overall |
Arlon 44580R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be used to wri.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Overall |
Arlon 30600R010 0.010" (0.254 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a Release Carrier Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Side 1 |
Arlon 30600R010 0.010" (0.254 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a Release Carrier Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Overall |
Arlon 44570R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Layers Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be use.. |