Polymer Property : Thickness = 100 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 254 - 2540 microns
10.0 - 100 mil
Range of thicknesses available
Rogers Corporation RT/duroid® 5880LZ Lightweight, High Frequency PTFE Laminate
RT/duroid® 5880LZ filled PTFE composites are designed for exacting stripline and microstrip circuit applications. The unique filler results in a low density, lightweight material for high performa..
Thickness 127 - 2540 microns
5.00 - 100 mil
Range of Standard Thicknesses
Rogers Corporation RT/duroid® 6006 Ceramic-PTFE Composite Microwave Laminate
Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowTight dielectric constant and thickness control for repeatable circuit performanceLow moi..
Thickness 127 - 2540 microns
5.00 - 100 mil
Range of Standard Thicknesses
Rogers Corporation RT/duroid® 6010.2LM Ceramic-PTFE Composite Microwave Laminate
Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowLow Z-axis expansion. Provides reliable plated through holes in multi-layer boardsTight ..