Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 180 - 1020 microns | 7.09 - 40.2 mil | |
Parker Chomerics CHO-BOND® 1016 Electrically Conductive Sealant Description: CHO-BOND 1016 sealant is an electrically conductive, one-component RTV silicone which provides both environmental sealing and EMI shielding. This seal, filled with nickel-plated graphit.. |
|||
Thickness | 180 - 12700 microns | 7.09 - 500 mil | |
Parker Chomerics Duralan II™ AR Polycarbonate Unshielded Window Description: Parker Chomerics display windows and filters are available in various plastic materials, including polycarbonate. A unique feature of Parker Chomerics window products is the capability.. |
|||
Thickness | 180 - 12700 microns | 7.09 - 500 mil | |
Parker Chomerics Duralan II™ P Polycarbonate Unshielded Window Description: Parker Chomerics display windows and filters are available in various plastic materials, including polycarbonate. A unique feature of Parker Chomerics window products is the capability.. |
|||
Thickness | 180 - 12700 microns | 7.09 - 500 mil | Average value: 4290 microns Grade Count:5 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Thickness | 180 microns | 7.09 mil | |
Isoflon Tisoflon® 6S Silicone Coated Glass Fabric Silicone coated Glass fabric TISOFLON®Information provided by Isoflon. |