Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 102 microns | 4.00 mil | |
Premix Thermoplastics PRE-ELEC® ESD 5500 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5500 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5500 can be injectio.. |
|||
Thickness | 102 microns | 4.00 mil | |
Premix Thermoplastics PRE-ELEC® ESD 6610 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6610 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6610 has b.. |
|||
Thickness | 102 microns | 4.00 mil | |
Premix Thermoplastics PRE-ELEC® PP 1394 Conductive Thermoplastic Compound PRE-ELEC® PP 1394 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Thickness | 102 microns | 4.00 mil | Liner |
Dielectric Polymers NT-100APS General Purpose Laminating Adhesive
(discontinued **) Acrylic adhesive with moisture stable PE coated kraft (60#) liner.Features: Plasticizer migration resistantChemical resistantMoisture resistantApplications: Mounting nameplates, signs, graphic panel.. |
|||
Thickness | 102 microns | 4.00 mil | |
Hexcel® HexForce™ 4527 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 102 microns | 4.00 mil | |
Dow Saran® 540 Clear Plastic Barrier Film Saran™ 540 is a clear biaxially oriented monolayer barrier film, designed for unit packaging and other applications. It is available in 4 gauge.Information provided by Dow |
|||
Thickness | 102 microns | 4.00 mil | Release Liner |
3M 1026 Adhesive Transfer Tape 3M™ Adhesive Transfer Tape 1026 is a 300 high strength acrylic adhesive on a 4 mil liner. Adhesive transfer tape in a pre-cut, tape strip on a pad.Features:5.0 mil adhesive transfer tape on a pad. .. |
|||
Thickness | 102 microns | 4.00 mil | Paper Liner |
3M 414DL Flexomount™ Solid Printing Tapes 3M™ Flexomount™ Solid Printing Tapes are double coated tapes designed for mounting photopolymer and rubber printing plates to flexographic printing cylinders or sleeve systems. The adhesive system.. |
|||
Thickness | 102 microns | 4.00 mil | Facestock |
3M 7052 Screen Printable Vinyl Performance Label Products 3M™ Screen Printable Vinyl Performance Label Products 7045 and 7052 are durable, high performance materials that offer good durability and moisture resistance. These vinyl label stocks utilize 3M™.. |
|||
Thickness | 102 microns | 4.00 mil | Release Liner |
3M 9420 Splicing Tapes 3M™ Splicing Tapes utilize on acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M |
|||
Thickness | 102 microns | 4.00 mil | Layer 1; Arlon SQA-TMS-003 |
Arlon 55589R032 0.034" (0.864 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 FiberglassAppearance: Red silicone gum and rubber on fiberglass This.. |
|||
Thickness | 102 microns | 4.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 56141R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass Side 1: Uncured Silicone Rubber This data represents typical values for the production m.. |
|||
Thickness | 102 microns | 4.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 56606R026 0.027" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production materia.. |
|||
Thickness | 102 microns | 4.00 mil | without adhesive |
3M Controltac™ 160 Graphic Film 4-mil, opaque white, opaque black and translucent white vinyl film with a matte finish; Pressure-activated adhesives for easy sliding, tacking, snap up and repositioning; Film series 160C-10 also ha.. |
|||
Thickness | 102 microns | 4.00 mil | without adhesive |
3M Controltac™ 8640C ES Graphic Film with Comply™ Adhesive This 4-mil film offers great versatility along with slidable, repositionable, pressure activated adhesive. This long term durable and removable film has excellent hiding power and stability, making .. |
|||
Thickness | 102 microns | 4.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon R34591R014 0.014" (0.356 mm) Uncured Silicone Rubber Design/Construction:Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 2116 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Appearance: Red silicon.. |
|||
Thickness | 102 microns | 4.00 mil | Facestock |
3M FM1142 Clear Polyester Label Products 3M™ Clear Polyester Label Products FM114N and FM1142 are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ Adhe.. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-24 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 microns | 4.00 mil | without adhesive |
3M Scotchcal™ IJ8171 Perforated Window Graphic Film Allows a full image to be seen on the outside while allowing viewing through windows from the inside; 4-mil, opaque vinyl film with a high gloss finish; White on the outside facing image side, black.. |
|||
Thickness | 102 microns | 4.00 mil | Wet |
3M Scotchkote™ MC 145 Epoxy Primer Scotchkote Epoxy Primer MC 145 is a solvent based two component primer suitable for use on a wide range of metallic and glass reinforced plastic (GRP) surfaces prior to the application of Scotchkote.. |
|||
Thickness | 102 microns | 4.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 51576R016A 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
Thickness | 102 microns | 4.00 mil | side 1; Arlon SQA-TMS-003 |
Arlon 51756R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber |
|||
Thickness | 102 microns | 4.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55146XA028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber This data represents typical values for the production mat.. |
|||
Thickness | 102 microns | 4.00 mil | Release Liner |
3M 950 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer adhesion to a wide variety of surfaces, including many plastics. This pressure-sensitive medium firm acrylic adhesive family features a very.. |
|||
Thickness | 102 - 152 microns | 4.00 - 6.00 mil | Side 1 |
Arlon R34260N005 0.005" (0.127 mm) Unsupported/Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Unsupported/Uncured Rubber Appearance: Clear gum on release linersThis data Represents typical values for the production material. The data should not be used to write, o.. |
|||
Thickness | 102 microns | 4.00 mil | without adhesive |
3M Controltac™ 3500C Changeable Graphic Film with Comply™ Adhesive 4-mil, opaque white vinyl film with a matte finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Air release channels for fast, easy, bub.. |
|||
Thickness | 102 microns | 4.00 mil | estimated wet film thickness |
Aremco Corr-Paint™ CP2000 High Temperature Protective Coating Urethane, Carbon Filled These epoxy and urethane based coatings are used for producing corrosion and wear resistant barriers to 500°F. Typical applications include tanks, piplines, boilers, precipitators, scrubbers, bag h.. |
|||
Thickness | 102 microns | 4.00 mil | Release Liner |
3M 466XL Extended Liner Tapes 3M™ Extended Liner Tapes have a liner that extends beyond the width of the adhesive to provide easy liner starting and removal. The liners, with the exception of 3M™ Extended Liner Tape 450EK is p.. |
|||
Thickness | 102 microns | 4.00 mil | Tape |
3M 9576 Splicing Tape 3M™ Splicing Tape offers excellent flying splice and core starting wet grab characteristics. They are typically used in the printing industry and perform well at process speeds in excess of 2000 fe.. |
|||
Thickness | >= 102 microns | >= 4.00 mil | Side 1 |
Arlon 44560R009W 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Appearance Red silicone gum on glass fabricThis data represents typical values for the production material. The data should not be used to write, .. |