Physical Properties Metric English Comments
Thickness 610 microns
24.0 mil
Fibre Glast 660 6K, 5HS Weave Carbon Fiber Fabric
Graphite fibers contain up to 95% carbon and yield the highest tensile strength in the FRP industry. These fibers woven together form graphite fabric. These fabrics offer higher strength and stiffne..
Thickness 610 microns
24.0 mil
Standard; Laminate
GrafTech GRAFOIL® GHH Standard Internal Combustion Laminate, Metal Reinforced
GRAFOIL® Grade GHH is a laminate made with GRAFOIL® Grade GTC flexible graphite chemically bonded to both faces of a flat, low-carbon steel core. Its applications include: exhaust sealing, ga..
Thickness 610 microns
24.0 mil
Nominal
DuPont™ Nomex® 410 Paper, 24 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..
Thickness 610 microns
24.0 mil
Overall; Arlon SQA-TMS-003
Arlon 51576R024A 0.024" (0.610 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat..
Thickness >= 610 microns
>= 24.0 mil
Side 2
Arlon 51586R035 0.035" (0.889 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mate..
Thickness 610 microns
24.0 mil
Side 1; Arlon SQA-TMS-003
Arlon 55142R040 0.040" (1.02 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass This data represents typical values for the production material. The data should not be use..
Thickness 610 microns
24.0 mil
Overall; Arlon SQA-TMS-003
Arlon 55572AA024 0.024" (0.610 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass This data represents typical values for the production material. The data should not be us..
Thickness 610 - 711 microns
24.0 - 28.0 mil
Overall
Arlon 56590R026 0.026" (0.660 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis data Represents typical values fo..
Thickness 610 - 711 microns
24.0 - 28.0 mil
Overall
Arlon 56606R026M 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass with polymer release li..
Thickness 610 - 660 microns
24.0 - 26.0 mil
Overall
Arlon P29609R025 0.025" (0.635 mm) Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Layer-on-Layer Product Use: Traction motor insulation, electrical insulationAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the pr..
Thickness 610 - 711 microns
24.0 - 28.0 mil
Overall
Arlon R34696R026 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o..
Thickness 610 microns
24.0 mil
Side 2 add-on thickness; Arlon SQA-TMS-003
Arlon R39118R037L 0.037" (0.940 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyester Release Liner Transfer Pressure Sensitive Adhesive: Silicone PSASide 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Cured Silicone Rubber..
Thickness 610 microns
24.0 mil
Overall Thickness; Arlon SQA-TMS-003
Arlon 55102R024 0.024" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production material and should not be used as material specifications.In..
Thickness 610 microns
24.0 mil
Overall; Arlon SQA-TMS-003
Arlon 55272R024 0.024" (0.610 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. The data should not be use..
Thickness 610 - 711 microns
24.0 - 28.0 mil
Overall
Arlon R33706R026 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass with polymer release li..