Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 6000 - 40000 microns | 236 - 1570 mil | |
Microtherm Group SlimVac Filament Reinforced Silica Vacuum Insulation Panel Microtherm® SlimVac panels are high performance evacuated microporous insulation panels covered in an impermeable outer envelope. The insulation is an opacified blend of filament reinforced silic.. |
|||
Thickness | 6000 microns | 236 mil | |
SMAC SMACWRAP® ST Damping Material, 0.60 mm SMACWRAP® concept is a smart and lightweight solution to embed into composite structures a very thin viscoelastic material. The SMACWRAP® will then bring damping to the composite structure wit.. |
|||
Thickness | 6000 microns | 236 mil | Standard(single pass) |
Trimay® Wear Plate T156 Iron-based Steel Overlay Overlay Description: T156 is a iron-based steel overlay wear solution with a unique proprietary chemical composition designed for moderate wear environments with moderate impact. T156 is similar to .. |
|||
Thickness | 6000 - 6500 microns | 236 - 256 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Thickness | 6000 - 6500 microns | 236 - 256 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness) AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Thickness | 6000 - 6500 microns | 236 - 256 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness) AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Thickness | 6000 - 6500 microns | 236 - 256 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness) AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Thickness | 6000 microns | 236 mil | |
American Computer Optics Low -Medium Transmission Filter 6 mm Maximum Size: 40" X 63"Abrasion: MIL-C-675C, section 4.5.11Adhesion: MIL-C-48497A, para 4.5.3.1Humidity: The coated optical surface will show no signs of deterioration after a 24 hour humidity expo.. |
|||
Thickness | 6000 microns | 236 mil | |
American Computer Optics Medium-High Transmission Filter 6 mm Maximum Size: 48" X 84"Abrasion: MIL-C-675C, section 4.5.11Adhesion: MIL-C-48497A, para 4.5.3.1Humidity: The coated optical surface will show no signs of deterioration after a 24 hour humidity expo.. |
|||
Thickness | 6000 microns | 236 mil | |
American Computer Optics Water White Filter 6 mm Maximum Size: 48" X 84"Abrasion: MIL-C-675C, section 4.5.11Adhesion: MIL-C-48497A, para 4.5.3.1Humidity: The coated optical surface will show no signs of deterioration after a 24 hour humidity expo.. |
|||
Thickness | 6000 microns | 236 mil | |
American Computer Optics Water White Filter 6 mm Single-Sided Maximum Size: 75" X 110"Abrasion: MIL-C-675C, section 4.5.11Adhesion: MIL-C-48497A, para 4.5.3.1Humidity: The coated optical surface will show no signs of deterioration after a 24 hour humidity exp.. |
|||
Thickness | 5990 microns | 236 mil | |
3M Scotchkote™ LW 405 Epoxy Concrete Mortar Scotchkote Epoxy Concrete Mortar LW 405 has been specifically developed as a three component 100% solids light weight repair mortar for use on concrete surfaces.Product Features:Designed for applica.. |
|||
Thickness | 6000 - 6500 microns | 236 - 256 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness) AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Thickness | 6000 - 6500 microns | 236 - 256 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (4.5 mm Molded Thickness) AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Thickness | 6000 microns | 236 mil | |
American Computer Optics High Transmission Filter 6 mm Maximum Size: 48" X 84"Abrasion: MIL-C-675C, section 4.5.11Adhesion: MIL-C-48497A, para 4.5.3.1Humidity: The coated optical surface will show no signs of deterioration after a 24 hour humidity expo.. |