Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 559 microns | 22.0 mil | cured, per ply |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 34-700 12K 2x2 Twill Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Thickness | 559 microns | 22.0 mil | nominal, cured, per ply |
Park Electrochemical Nelcote® F-562 Phenolic Prepreg, 8HS Silica Reinforced Nelcote® F-562 is an elastomer modified phenolic resin used in the manufacture of intermediate temperature ablative rocket nozzles, heat shields and combustion chambers in highly oxidative environm.. |
|||
Thickness | 559 microns | 22.0 mil | Gauge, nominal |
Mid-Mountain Materials ARMATEX® SF22 Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Thickness | 560 microns | 22.0 mil | 120 |
LATI Latigray 82-02 CX/80 PA 12 Radiopaque compound based on Polyamide 12 (PA12). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Thickness | 559 - 711 microns | 22.0 - 28.0 mil | Overall |
Arlon 51570R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to wri.. |
|||
Thickness | 559 microns | 22.0 mil | Tape |
3M Cushion-Mount™ 1020R Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 559 microns | 22.0 mil | Tape |
3M Cushion-Mount™ 1820M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 559 microns | 22.0 mil | Tape |
3M Cushion-Mount™ 1920S Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 559 microns | 22.0 mil | Tape |
3M Cushion-Mount™ E1020 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 559 microns | 22.0 mil | Tape |
3M Cushion-Mount™ E1120 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 559 microns | 22.0 mil | Tape |
3M Cushion-Mount™ E1220 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 559 microns | 22.0 mil | Tape |
3M Cushion-Mount™ E1520 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 559 microns | 22.0 mil | Tape |
3M Cushion-Mount™ E1820 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 559 microns | 22.0 mil | Tape |
3M Cushion-Mount™ E1915S Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 559 microns | 22.0 mil | Side 2; Arlon SQA-TMS-003 |
Arlon R36386C035 0.035" (0.889 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber (Ferromagnetic Filler) Substrate: Style 7628 Fiberglass This data represents typical value.. |
|||
Thickness | 559 microns | 22.0 mil | Side 1 |
Arlon 55503R062 0.062" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Prime Coated 162 Style FiberglassSide 2: Cured Silicone RubberThis data represents typical values for th.. |
|||
Thickness | 559 microns | 22.0 mil | Side 2 |
Arlon 55503R062 0.062" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Prime Coated 162 Style FiberglassSide 2: Cured Silicone RubberThis data represents typical values for th.. |
|||
Thickness | 559 microns | 22.0 mil | Tape |
3M Cushion-Mount™ 1020 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 559 microns | 22.0 mil | Tape |
3M Cushion-Mount™ 1020M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 559 microns | 22.0 mil | Tape |
3M Cushion-Mount™ E1920S Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 560 microns | 22.0 mil | |
3M Nextel™ XN-625 Woven Fabric 720 Information provided by 3M |
|||
Thickness | 559 microns | 22.0 mil | Tape |
3M Cushion-Mount™ 1120 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 559 microns | 22.0 mil | Tape |
3M Cushion-Mount™ 1120K Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 559 microns | 22.0 mil | Tape |
3M Cushion-Mount™ 1720M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 559 microns | 22.0 mil | Tape |
3M Cushion-Mount™ 1920M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 559 microns | 22.0 mil | Tape |
3M Cushion-Mount™ E1320 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 559 microns | 22.0 mil | Tape |
3M Cushion-Mount™ E1720 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 559 microns | 22.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R36613N022 0.022" (0.559 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 7628 Heat Cleaned FiberglassSide 2: Cured Silicone RubberSide 2 Interleave: PolyethyleneFiberglas Weave: PlainThis data represents.. |