Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 508 - 1500 microns | 20.0 - 59.0 mil | Range of Thicknesses Available |
Rogers Corporation Poron® 4790-92-12 P Series Urethane Foam, Extra Soft, Slow Rebound, PET Film Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Thickness | 508 microns | 20.0 mil | overall; Arlon SQA-TMS-003 |
Arlon A3020-B004-12 Silicone Rubber/Fiberglass Laminate
(discontinued **) Side 1: cured fusible silicone rubber; Substrate: 25% sinusoidal fiberglass; Side 2: cured fusible silicone rubber; Interleave: 1 mil PE film |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 31580R020 0.020" (0.508 mm) Uncured Silicone Rubber on HDPE Carrier
(discontinued **) Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: High Density PolyethyleneAppearance: Red silicone gum on polymer linerThis data represents typical values for the.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R34710R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l Description: 20 mil thick uncured, uncatalyzed silicone rubber. Used for sealing biochemical reaction chambers.Design/Construction:Liner: Polyethylene Product: Uncured Silicone Rubber Carrier: Mylar.. |
|||
Thickness | 508 microns | 20.0 mil | |
GrafTech eGRAF® HITHERM™ HT-720 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Thickness | 508 microns | 20.0 mil | |
GrafTech eGRAF® HITHERM™ HT-1220 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Thickness | 508 microns | 20.0 mil | Nominal |
DuPont™ Nomex® E56 Paper, 20 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 10502R020 0.020" (0.508 mm) Cured Silicone Rubber (Unsupported) Design/Construction:Material: Cured Silicone RubberLiner: Polyethylene Recommended Cure Cycle: Product delivered curedRecommended Post Cure Cycle: Product delivered post-curedAppearance: Red silicon.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 19540R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 1523 Style FiberglassThis data represents typical values for the production material. The data should not be u.. |
|||
Thickness | 508 - 610 microns | 20.0 - 24.0 mil | Overall |
Arlon 30090R022 0.022" (0.559 mm) Uncured Unsupported Silicone Rubber on Kodacel Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Kodacel Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The d.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 32580R020 0.020" (0.508 mm) Uncured Silicone Rubber on Polyester Film Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmAppearance: Red silicone gum on polymer linerThis data represents typical values for the production.. |
|||
Thickness | 508 microns | 20.0 mil | overall; Arlon SQA-TMS-003 |
Arlon 51106RB015D Silicone Rubber/Fiberglass Laminate Interleave 2: 3 mil PE; Side 2: cured silicone rubber; Substrate: 7628 fiberglass; Side 1: uncured silicone rubber, Interleave 1: 3 mil PE |
|||
Thickness | 508 microns | 20.0 mil | Overall Thickness |
Arlon 51422R020 0.020" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Prime Coated 7628 FiberglassInterleave: 3 mil PolyethyleneThis data represents typical values for the production material and should no.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-012 |
Arlon 920-05C##FR-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 0.5” Wide Rectangular .0.5 inch wide, 20 mil thick, Black, Rectangular cross-section, Se.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 920-10R##-P2 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Red, Rectangular cross-section, Self-fusi.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 920-10T##-P0 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Transparent, Rectangular cross-section, S.. |
|||
Thickness | 508 microns | 20.0 mil | Rubber; Arlon SQA-TMS-012 |
Arlon LW201R##-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: Level Wrap®: 1 inch wide, 20 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R30711R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1165 Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: PolyethyleneAppearance: Red silicone gum .. |
|||
Thickness | 508 microns | 20.0 mil | Product; Arlon SQA-TMS-003 |
Arlon R34710R020 0.020" Uncured Silicone Rubber with Mylar Carrier 20 mil thick, uncured, uncatalyzed silicone rubber. Used for sealing biochemical reaction chambers.Design/Construction:Liner: 3 mil Pink PEProduct: Uncured Silicone RubberCarrier: MylarThis data.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon T2020-R004 0.020" (0.508 mm) Cured Self-Fusing Silicone Rubber Description: 1 inch wide x 20 mil thick, Black, Triangular cross-section, Self-Fusing Silicone TapeDesign/Construction: Interleave: Polyethylene Product: Cured Self-Fusing Silicone RubberCross-Secti.. |
|||
Thickness | 508 microns | 20.0 mil | Overall thickness; Arlon SQA-TMS-012 |
Arlon T3020-B004 0.020" Self-Fusing, Cured Silicone Rubber Tape with Fiberglass Substrate 1.0 inch wide, 20 mil thick, black, rectangular cross-section, self-fusing silicone tape.Design/Construction:Side 1: Cured Silicone RubberSubstrate: 25% Sinusoidal FiberglassSide 2: Cured Silicone.. |
|||
Thickness | 508 microns | 20.0 mil | |
3M Scotchkote™ 80BG 536 Urethane Elastomer Scotchkote Urethane Elastomer 80BG 536 has been specifically developed as an elastomeric system with a high degree of flexibility for resurfacing rubber components. Product Features:Properties simil.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 31570R020 0.020" (0.508 mm) Uncured Silicone Rubber on Release Carrier Design/Construction: Interleave: PolyethyleneProduct: Uncured Silicone Rubber Release Carrier: HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the pr.. |
|||
Thickness | 508 microns | 20.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 32580X030 0.030" (0.762 mm) Uncured Unsupported Silicone Rubber on a PET Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on PET CarrierAppearance: Gray silicone gum on polymer linerThis data represents typical values for the production material. The data .. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 51231R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical .. |
|||
Thickness | 508 microns | 20.0 mil | Silicone |
Arlon 41580R020 0.020" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 44141R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Clear PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Blue PolyethyleneThis data represent.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 44602W020W 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 1165 FiberglassProduct is designed to meet the FAR 25.853 App.F, P.1,.Aii flame resistance requirements b.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 31140R020 0.020" (0.508 mm) Uncured Fluorosilicone Rubber on Release Carrier Design/Construction: Interleave: PolyethyleneProduct: Uncured Fluorosilicone Rubber Carrier: Release coated HDPE Product Use: Flexible heater insulationAppearance: Red silicone gum on polymer releas.. |