Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 61.0 microns | 2.40 mil | |
Hexcel® HexForce™ 1280 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 61.0 microns | 2.40 mil | ExxonMobil Method |
ExxonMobil Label-Lyte™ 60ZH247 OPP Film Product Description: A super white opaque, caviated BOPP film for Pressure Sensitive (PSA) labeling applications where good optical properties are required. 60ZH247 also shows excellent performances.. |
|||
Thickness | 61.0 microns | 2.40 mil | ExxonMobil Method |
ExxonMobil Label-Lyte™ 70LTR742 OPP Film Product Description: A matte finish, coated, white, polypropylene film designed for use in demanding thermal transfer, pressure-sensitive label applications. It is also compatible with a wide range .. |
|||
Thickness | 61.0 microns | 2.40 mil | ExxonMobil Method |
ExxonMobil Oppalyte™ 60MH247 OPP Film Product Description: A super white opaque, modified higher density, biaxially oriented PP film. This opaque and stiff film is ideal for mono material requirements and it has been designed for cold s.. |
|||
Thickness | 61.0 microns | 2.40 mil | Total; ASTM D3652 |
3M 3369 General Purpose Aluminum Foil Tape Thinnest aluminum foil tape. UL 723 Classified.Information provided by 3M |
|||
Thickness | 61.0 microns | 2.40 mil | Glass Cloth Backing; ASTM D3752 |
3M 363LC High Temperature Aluminum Foil/Glass Cloth Tape 3M™ High Temperature Aluminum Foil/Glass Cloth Tape 363LC can be used as a high temperature, heat reflective, protective wrap for certain cables and other components in aerospace and industrial app.. |
|||
Thickness | 61.0 microns | 2.40 mil | Total; ASTM D3752 |
3M 616 Lithographers Tape 3M™ Lithographers Tape 616 is an optically transparent and photographically opaque tape.Information provided by 3M |
|||
Thickness | 61.0 microns | 2.40 mil | Total; ASTM D3752 |
3M 8991 Polyester Tape 3M™ Polyester Tape 8991 is a blue polyester tape with a silicone adhesive. It can be used in a large variety of high temperature applications including powdercoat masking, flashbreaker, and bag sea.. |
|||
Thickness | 61.0 microns | 2.40 mil | Backing |
3M CN-3490 EMI Shielding Tape 3M EMI Shielding Tapes are well suited for applications requiring reliable point-to-point electrical contact, particularly EMI shielding, grounding and static charge draining.Information provided by.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FM011 Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FM452 Indoor UL Recognized Clear Polyester Overlaminate Label Products 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FM691 Indoor UL Recognized Computer Imprintable Clear Polyester Label Product 3M™ Indoor UL Recognized Computer Imprintable Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FP022101 White Polypropylene Label Product 3M™ White Polypropylene Label Products FP022101, FP022102, FP022108, FP026002, FP02600N and FP026009 are matte white opaque materials that offer excellent durability and moisture resistance. These .. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FP024901 White Polypropylene Label Products 3M™ White Polypropylene Label Products are matte white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a general.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FP08R2 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FP101 Clear Polypropylene Label Product 3M™ Clear Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1410, which is a general purpose permanent tackified acrylic t.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FP531 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FV091 Soft Translucent Vinyl Label Products 3M™ Soft Translucent Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FV291 White Vinyl Label Products 3M™ White Vinyl Label Products FV291 and FV292 are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl label products utilize 3M™ Adhesive P14.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M OFM0101 Outdoor UL Recognized Polyester Overlaminate Label Products 3M™ Outdoor UL Recognized Polyester Overlaminate Label Products are durable high performance clear materials that offer excellent thermal stability, abrasion and moisture resistance. These polyeste.. |
|||
Thickness | 61.0 microns | 2.40 mil | estimated wet film thickness |
Aremco Corr-Paint™ CP4010-S1 High Temperature Protective Coating, Silicone |
|||
Thickness | 61.0 microns | 2.40 mil | estimated wet film thickness |
Aremco HiE-Coat™ 840-MS High Emissivity Silicone-Ceramic Coating 840-C is a silicone-ceramic, black-pigmented coating for aluminum, brass, copper, and carbon and stainless steels to 1100 ºF (593 ºC).The HiE-Coat™ line of high emissivity coatings are black-body.. |
|||
Thickness | 61.0 microns | 2.40 mil | Total; ASTM D3752 |
3M 8901 Polyester Tape 3M™ Polyester Tape 8901 is made with strong polyester backing and silicone adhesive, allowing it to be used in applications requiring high temperatures or adhesion to silicone treated surfaces. Thi.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FA031 Matte Clear Acetate Label Products 3M™ Matte Clear Acetate Label Products offer consistent, high quality film appearance. This film die-cuts easily which helps extend die life in comparison with polyester label stocks. These acetate.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FM1541 Clear Polyester Label Products 3M™ Clear Polyester Label Products FM1541 and FM1542 are durable, high performance materials that offer excellent thermal stability and moisture resistance. These label products utilize 3M™ Adhesi.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FM291 Indoor UL Recognized Clear Polyester Overlaminate Label Products 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FS501 White Polystyrene Label Products 3M™ White Polystyrene Label Products FS501, FS502 and FS532 are hard, rigid film materials that offer economic alternatives for indoor applications. These polystyrene labels utilize 3M™ Adhesive R.. |
|||
Thickness | 61.0 microns | 2.40 mil | estimated wet film thickness |
Aremco Cerama-Dip™ 538-N High Temperature Specialty Ceramic-Inorganic Coating Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available. |
|||
Thickness | 61.0 microns | 2.40 mil | estimated wet film thickness |
Aremco Corr-Paint™ CP4010 High Temperature Protective Silicone Coating, Aluminum Filled Single part, silicone-based, low viscosity, heat-curable, aluminum-filled sealer offering exceptional moisture resistance to 1100°F (593°C). |
|||
Thickness | 61.0 microns | 2.40 mil | Total; ASTM D3752 |
3M 8991L Polyester Tape 3M™ Polyester Tape 8991L is a blue polyester tape with a silicone adhesive. It can be used in a large variety of high temperature applications including powdercoat masking, flashbreaker, and bag se.. |