Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 3000 - 3510 microns | 118 - 138 mil | |
Zircar Zirconia ZYF-A2.13 Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |
|||
Thickness | >= 3000 microns | >= 118 mil | plus or minus 100 microns |
GrafTech GRAFCELL® FFP-300 SERIES Flow Field Plate Graphite Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid.. |
|||
Thickness | 3000 microns | 118 mil | |
Sylvin Technologies 916V0 Black PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Thickness | 3000 microns | 118 mil | |
Eastman Spectar® 14471 Copolyester Spectar copolyester extrudes into plastic sheet that is sparkling clear, tough, chemically resistant, odor-free, versatile, easy to work with and affordable. Its toughness allows fabricators to use .. |
|||
Thickness | 3000 microns | 118 mil | |
Eastman Spectar® Clear Copolyester for Thermoforming Applications:Decorative Light-Transmitting PanelsHeavy gauge sheet displaysKey Attributes:Easy to print and decorateExcellent clarityExcellent thermoforming characteristicsGood chemical resistanceOd.. |
|||
Thickness | 3000 microns | 118 mil | |
Eastman TiGlaze SV Copolyester TiGLAZE SV copolyester is a specialty copolyester for the architectural glazing industry, designed to provide a unique balance of toughness, stiffness and material value. The material has a CC1 Ligh.. |
|||
Thickness | 3000 microns | 118 mil | |
American Computer Optics 12.1in Tempered LCD Glass Maximum Size: 8.2" X 10.6"Abrasion: MIL-C-675C, section 4.5.11Adhesion: MIL-C-48497A, para 4.5.3.1Humidity: The coated optical surface will show no signs of deterioration after a 24 hour humidity e.. |
|||
Thickness | 3000 microns | 118 mil | |
American Computer Optics 17in Tempered LCD Glass Maximum Size: 11.46" X 14.16"Abrasion: MIL-C-675C, section 4.5.11Adhesion: MIL-C-48497A, para 4.5.3.1Humidity: The coated optical surface will show no signs of deterioration after a 24 hour humidit.. |
|||
Thickness | 3000 microns | 118 mil | |
American Computer Optics 18in Tempered LCD Glass Maximum Size: 12.15" X 15.28"Abrasion: MIL-C-675C, section 4.5.11Adhesion: MIL-C-48497A, para 4.5.3.1Humidity: The coated optical surface will show no signs of deterioration after a 24 hour humidit.. |
|||
Thickness | 3000 microns | 118 mil | |
American Computer Optics Low -Medium Transmission Filter 3 mm Maximum Size: 31" X 34"Abrasion: MIL-C-675C, section 4.5.11Adhesion: MIL-C-48497A, para 4.5.3.1Humidity: The coated optical surface will show no signs of deterioration after a 24 hour humidity expo.. |
|||
Thickness | 3000 microns | 118 mil | |
American Computer Optics Water White Filter 3 mm Single-Sided Maximum Size: 75" X 110"Abrasion: MIL-C-675C, section 4.5.11Adhesion: MIL-C-48497A, para 4.5.3.1Humidity: The coated optical surface will show no signs of deterioration after a 24 hour humidity exp.. |
|||
Thickness | 3000 microns | 118 mil | Mastic-Pad; ASTM D1000 |
3M Scotch™ 2200 Vinyl Mastic Pads and Rolls 3M™ Scotch™ Brand 2200 Pads and 2210 Rolls are self fusing, rubber based insulating compounds laminated to a flexible, all weather grade vinyl (PVC) backing. These tape rolls and precut pads are d.. |
|||
Thickness | 3000 microns | 118 mil | Mastic-Pad; ASTM D1000 |
3M Scotch™ 2210 Vinyl Mastic Pads and Rolls 3M™ Scotch™ Brand 2200 Pads and 2210 Rolls are self fusing, rubber based insulating compounds laminated to a flexible, all weather grade vinyl (PVC) backing. These tape rolls and precut pads are d.. |
|||
Thickness | >= 3000 microns | >= 118 mil | |
Beijing Evergrow Resources GFF-3 Glass Fiber Felt Introduction:By applying high-count fiberglass, GFNF series has the excellent properties such as heat-isolation, fire-resistance, anti-corrosion and heat-preservation. It's the most characteristic a.. |
|||
Thickness | 3000 - 30000 microns | 118 - 1180 mil | |
Beijing Evergrow Resources Polyurethane Activated Carbon Features:good strengthgood flexilitygood durabilityApplications:Air purificationInformation provided by Beijing Evergrow Resources. |
|||
Thickness | 3000 microns | 118 mil | |
American Computer Optics Low Transmission Filter 3 mm Maximum Size: 40" X 63"Abrasion: MIL-C-675C, section 4.5.11Adhesion: MIL-C-48497A, para 4.5.3.1Humidity: The coated optical surface will show no signs of deterioration after a 24 hour humidity expo.. |
|||
Thickness | 3000 - 4000 microns | 118 - 157 mil | |
Beijing Evergrow Resources BF-3 Basalt Needle Felt Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi.. |