Physical Properties Metric English Comments
Thickness 32.3 microns
1.27 mil
Cured Ply Thickness: HexTOOL™ M61 (2000); Based on nominal prepreg properties
Hexcel® HexTOOL™ M61 Quasi-isotropic High Temperature Prepreg Tooling Compound
HexTOOL™ Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequentl..