Polymer Property : Thickness = 0.433 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 11.0 - 13.0 microns
0.433 - 0.512 mil
Fired
Lord Adhesives Metech 1130C Platinum Silver Conductor Composition
This low cost, platinum silver conductor is designed for general hybrid applications. It employs advanced powders technology with a mix bonded frit system to yield a highly dense film that is resist..
Thickness 11.0 - 13.0 microns
0.433 - 0.512 mil
Fired
Lord Adhesives Metech 3524 Silver Conductor Composition
This silver conductor composition is designed for screen printing applications requiring nickel barrier plating. It fires to a highly dense film which is resistant to acidic plating solutions.All in..
Thickness 11.0 - 13.0 microns
0.433 - 0.512 mil
Fired
Lord Adhesives Metech 3571 Silver Conductor Composition
This high performance silver conductor is designed for cost sensitive hybrid applications. It employs advanced powders technology with a mix bonded frit system to yield a highly dense fired film tha..
Thickness 11.0 - 13.0 microns
0.433 - 0.512 mil
Fired
Lord Adhesives Metech 3524D Silver Conductor Composition
This silver conductor composition is designed for machine-dipped edge termination applications requiring nickel barrier plating. It fires to a highly dense film which is resistant to acidic plating ..