Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 25.0 - 80.0 microns | 0.984 - 3.15 mil | Recommended |
Polimeri Europa Riblene® FL 20 Low Density Polyethylene - Blown Film Extrusion Riblene FL 20 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FL 20 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
Thickness | 25.0 - 80.0 microns | 0.984 - 3.15 mil | Recommended |
Polimeri Europa Riblene® FL 23 Low Density Polyethylene - Blown Film Extrusion Riblene FL 23 is a low density polyethylene (LDPE) with added slip agent, suitable for blown film extrusion. Riblene FL 23 is characterized by a good balance between processability and mechanical p.. |
|||
Thickness | 25.0 - 80.0 microns | 0.984 - 3.15 mil | Recommended |
Polimeri Europa Riblene® FL 24 Low Density Polyethylene - Blown Film Extrusion Riblene FL 24 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 24 is characterized by a good balance between processabilit.. |
|||
Thickness | 25.0 - 80.0 microns | 0.984 - 3.15 mil | Recommended |
Polimeri Europa Riblene® FL 30 Low Density Polyethylene - Blown Film Extrusion Riblene FL 30 is a low density polyethylene (LDPE) ideal for blown film extrusion. Riblene FL 30 is characterized by a good balance between processability, mechanical and optical properties.Films m.. |
|||
Thickness | 25.0 - 80.0 microns | 0.984 - 3.15 mil | Recommended |
Polimeri Europa Riblene® FL 34 E Low Density Polyethylene - Blown Film Extrusion Riblene FL 34 E is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 34 E is characterized by a good balance between processab.. |
|||
Thickness | 25.0 - 80.0 microns | 0.984 - 3.15 mil | Recommended |
Polimeri Europa Riblene® FL 34 Low Density Polyethylene - Blown Film Extrusion Riblene FL 34 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 34 is characterized by a good balance between processabilit.. |
|||
Thickness | 40.0 - 80.0 microns | 1.57 - 3.15 mil | |
Möller Medical PolySkin 98 S NanoCoating Flexible, non-abrasive "soft feel" coating with velour-like surface.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Thickness | 40.0 - 80.0 microns | 1.57 - 3.15 mil | |
Indium Corp. NanoFoil® NF40 Nickel and Aluminum Localized Heat Source For Bonding Features:40 microns thick - optimized for bonding electronics assembliesMinimum dimension 1.2mm x 2.0mmLocalized heat source for bondingEnables high-strength, high conductivity bonds between most co.. |
|||
Thickness | 30.0 - 80.0 microns | 1.18 - 3.15 mil | |
Daikin NEOFLON ACX-31 PFA Coating Powder, White NEOFLON PFA coating powder is designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 30-80 micron thickness.Processing Methods: Electrostati.. |
|||
Thickness | 30.0 - 80.0 microns | 1.18 - 3.15 mil | |
Daikin NEOFLON ACX-34 PFA Coating Powder, White NEOFLON PFA coating powder is designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 30-80 micron thickness.Processing Methods: Electrostati.. |
|||
Thickness | 70.0 - 80.0 microns | 2.76 - 3.15 mil | |
CEN® Electronic Material CN Polyimide Film, 3 Mil Thickness CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca.. |
|||
Thickness | 70.0 - 80.0 microns | 2.76 - 3.15 mil | ASTM D374 |
CEN® Electronic Material CV Polyimide Film, 3 Mil Thickness CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup.. |