Physical Properties Metric English Comments
Thickness 6000 - 6500 microns
236 - 256 mil
Typical free lofted thickness after heating
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness)
AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Thickness 6000 - 6500 microns
236 - 256 mil
Typical free lofted thickness after heating
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness)
AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Thickness 6000 - 6500 microns
236 - 256 mil
Typical free lofted thickness after heating
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness)
AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Thickness 6000 - 6500 microns
236 - 256 mil
Typical free lofted thickness after heating
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness)
AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Thickness 6000 - 6500 microns
236 - 256 mil
Typical free lofted thickness after heating
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness)
AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Thickness 6000 - 6500 microns
236 - 256 mil
Typical free lofted thickness after heating
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (4.5 mm Molded Thickness)
AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..