Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 50.0 - 200 microns | 1.97 - 7.87 mil | Recommended |
Polimeri Europa Greenflex® FC 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FC 45 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FC 45 exhibit good optical properties, excellent impact resistance and low creep.. |
|||
Thickness | 175 - 200 microns | 6.89 - 7.87 mil | |
Parker Chomerics WIN-SHIELD® AgF8 Conductive Film Description: Chomerics’ AgF8 conductive film is a multi-layer, silver oxide-based thin film coating applied to a heat stabilized, optical quality polyester film AgF8 film-provides high visible ligh.. |
|||
Thickness | 50.0 - 200 microns | 1.97 - 7.87 mil | Recommended |
Polimeri Europa Greenflex® FD 20 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 20 is an ethylene vinyl acetate copolymer (EVA) suitable for blown film extrusion. Films produced with Greenflex FD 20 exhibit good optical properties, high impact resistance, tensile .. |
|||
Thickness | 50.0 - 200 microns | 1.97 - 7.87 mil | Recommended |
Polimeri Europa Greenflex® FD 23 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 23 is an ethylene vinyl acetate copolymer (EVA) suitable for blown film extrusion. Greenflex FD 23 is a version of Greenflex FD 20 with added slip and antiblocking agents. Films produ.. |
|||
Thickness | 50.0 - 200 microns | 1.97 - 7.87 mil | Recommended |
Polimeri Europa Greenflex® FD 50 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 50 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FD 50 exhibit good optical and sealing properties, high flexibility and toughnes.. |
|||
Thickness | 50.0 - 200 microns | 1.97 - 7.87 mil | Recommended |
Polimeri Europa Greenflex® FD 53 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 53 is an ethylene vinyl acetate copolymer (EVA), containing antiblocking agent, for blown film extrusion. Films produced with Greenflex FD 53 exhibit good sealing properties, high flex.. |
|||
Thickness | 30.0 - 200 microns | 1.18 - 7.87 mil | possible range, depending on extrusion conditions |
Total EVA 1005 VN 35 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 35 is made by a high pressure tubular process. Grade for flexible films, with high transparency and outstanding mechanical properties. Contains NO antioxidant.Information provided by T.. |
|||
Thickness | 50.0 - 200 microns | 1.97 - 7.87 mil | |
Bapolene® 105F Low Density Polyethylene Film Resin Description: Bapolene LD105F is an unmodified low density polyethylene which extrudes into a low gloss high impact film. It contains antiblock additives and no slip additives. This product meets th.. |
|||
Thickness | 120 - 200 microns | 4.72 - 7.87 mil | |
Beijing Evergrow Resources CFC-DD-1000 Carbon Fiber Cloth The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro.. |
|||
Thickness | 120 - 200 microns | 4.72 - 7.87 mil | |
Beijing Evergrow Resources CFC-DD-1000S Carbon Fiber Cloth The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro.. |
|||
Thickness | 120 - 200 microns | 4.72 - 7.87 mil | |
Beijing Evergrow Resources CFC-DDX-1000S Carbon Fiber Cloth The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro.. |
|||
Thickness | 65.0 - 200 microns | 2.56 - 7.87 mil | |
Caplinq LINQSTAT™ VCF-40006T/2 Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Thickness | 65.0 - 200 microns | 2.56 - 7.87 mil | |
Caplinq LINQSTAT™ VCF-40006T/4 Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Thickness | 65.0 - 200 microns | 2.56 - 7.87 mil | |
Caplinq LINQSTAT™ VCF-40009.5S/2 Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Thickness | 65.0 - 200 microns | 2.56 - 7.87 mil | |
Caplinq LINQSTAT™ VCF-40012T/2 Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Thickness | 65.0 - 200 microns | 2.56 - 7.87 mil | |
Caplinq LINQSTAT™ VCF-40036S/2 Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Thickness | 65.0 - 200 microns | 2.56 - 7.87 mil | |
Caplinq LINQSTAT™ VCF-40054V/2 Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Thickness | 65.0 - 200 microns | 2.56 - 7.87 mil | |
Caplinq LINQSTAT™ VCF-40406B Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Thickness | 65.0 - 200 microns | 2.56 - 7.87 mil | |
Caplinq LINQSTAT™ VCF-40810B Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Thickness | 65.0 - 200 microns | 2.56 - 7.87 mil | |
Caplinq LINQSTAT™ VCF-41014B Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Thickness | 65.0 - 200 microns | 2.56 - 7.87 mil | |
Caplinq LINQSTAT™ VCF-42424B Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Thickness | 65.0 - 200 microns | 2.56 - 7.87 mil | |
Caplinq LINQSTAT™ VCF-43036B Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Thickness | 65.0 - 200 microns | 2.56 - 7.87 mil | |
Caplinq LINQSTAT™ VCF-80036S/2 Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Thickness | 120 - 200 microns | 4.72 - 7.87 mil | |
Beijing Evergrow Resources CFC-DDX-1000 Carbon Fiber Cloth The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro.. |
|||
Thickness | 65.0 - 200 microns | 2.56 - 7.87 mil | |
Caplinq LINQSTAT™ VCF-40054V/m Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |