Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 3.00 - 10.0 microns | 0.118 - 0.394 mil | |
Möller Medical NanoSkin Magic 101 L NanoCoating Conducting coating with very good chemical resistance, biocompatible, becoming hydrophilic after water contactInformation provided by Möller Medical, Member of CENTROTEC Group |
|||
Thickness | 1.00 - 10.0 microns | 0.0394 - 0.394 mil | |
Möller Medical PolySkin 102 M NanoCoating Decorative, thermally stable coating with "metallic look," easy-to-clean effect can be added.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Thickness | 3.00 - 10.0 microns | 0.118 - 0.394 mil | |
Möller Medical PolySkin 78 M NanoCoating Decorative coating in "metallic look," hardening at room temperature up to 80°C.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Thickness | 2.00 - 10.0 microns | 0.0787 - 0.394 mil | |
Möller Medical TafSkin 109 L NanoCoating Electrically conducting, chemical-resistant, thin, easy-to-clean PTFE coatingInformation provided by Möller Medical, Member of CENTROTEC Group |
|||
Thickness | 7.00 - 10.0 microns | 0.276 - 0.394 mil | Fired |
Lord Adhesives Metech 3614 Gold Conductor Gold conductor composition 3614 is a thin print, mixed bond conductor. It has been formulated for both inner layer use in multilayer hybrids as well as for smooth, flat wire bond pads to optimize yi.. |
|||
Thickness | 6.00 - 10.0 microns | 0.236 - 0.394 mil | |
Eifeler Coatings Technology TiC/TiN CVD Coating The titanium carbide/titanium nitride combination layer is a standard layer well-proven over a long time. Layer properties: Very high hardness; Very good adhesion; Sufficient toughnessInforma.. |
|||
Thickness | 7.00 - 10.0 microns | 0.276 - 0.394 mil | |
Eifeler Coatings Technology TiN/TiC CVD Coating The titanium nitride / titanium carbide combination layer is a standard layer well-proven over a long time. It indicates the following properties: Very high hardness; Very good adhesion; Suffic.. |
|||
Thickness | 5.00 - 10.0 microns | 0.197 - 0.394 mil | |
Eifeler Coatings Technology TOPMATIC TiAlN PVD Coating This layer on the basis of TiAlN is relatively tough and can therefore be deposited in comparably high layer thicknesses. The adhesion of the coating is outstanding.Information provided by Eifeler C.. |