Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 889 microns | 35.0 mil | Gauge, nominal |
Mid-Mountain Materials ARMATEX® SF32 Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Thickness | 889 microns | 35.0 mil | Gauge, nominal |
Mid-Mountain Materials ARMATEX® SF37 Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Thickness | 889 - 1650 microns | 35.0 - 65.0 mil | |
Zircar Zirconia ZYF-50 Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |
|||
Thickness | 889 - 1040 microns | 35.0 - 41.0 mil | Side 1 |
Arlon 25122R040 0.040" (1.02 mm) Silicone Rubber on Laminated Fluoropolymer Film Appearance: Red silicone rubber chemically bonded to fluoropolymer filmThis data represents typical values for the production material. The data should not be used to write, or in place of, material.. |
|||
Thickness | 889 microns | 35.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 32580B035 0.035" (0.889 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETThis data represents typical values for the production material. The data should not be used to write, or in p.. |
|||
Thickness | 889 microns | 35.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 32580B035 0.035" (0.889 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETThis data represents typical values for the production material. The data should not be used to write, or in p.. |
|||
Thickness | 889 microns | 35.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 32580R035 0.035" (0.889 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. .. |
|||
Thickness | 889 microns | 35.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 32580R035 0.035" (0.889 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. .. |
|||
Thickness | 889 microns | 35.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R36386C035 0.035" (0.889 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber (Ferromagnetic Filler) Substrate: Style 7628 Fiberglass This data represents typical value.. |
|||
Thickness | 889 - 1090 microns | 35.0 - 43.0 mil | Overall |
Arlon R34332X039 0.039" (0.991 mm) Fully Cured/Unsupported Design/Construction:Overall: Fully cured/unsupported This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.In.. |
|||
Thickness | 889 microns | 35.0 mil | Wet |
3M Scotchkote™ 136 Encapsulation Coating Polynox Scotchkote Encapsulation Coating Polynox 136 is a water based acrylic anti corrosive coating specifically developed to provide long term protection and encapsulation of previously coated structures... |
|||
Thickness | 889 microns | 35.0 mil | Total Thickness |
3M 9593 Double Coated Tapes with Adhesive 350 3M™ Double Coated Tapes 9500PC, 9500B, 9593 and 3028EK feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. 3M™ Adhesive 350 is a .. |
|||
Thickness | 889 - 1650 microns | 35.0 - 65.0 mil | |
Zircar Zirconia ZYF-50 Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |