Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 88.9 microns | 3.50 mil | Total; ASTM D1000 |
Parker Chomerics CHO-JAC CJ-022 Flat Cable EMI Shield Flat Cable EMI Shield. Cho-Jack® shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into compliance with FCC and TEMPEST radiated em.. |
|||
Thickness | 88.9 microns | 3.50 mil | |
Hexcel® HexForce™ 220HT Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 88.9 microns | 3.50 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 28561R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1528 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum o.. |
|||
Thickness | 88.9 microns | 3.50 mil | Side 1 |
Arlon 49576R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mat.. |
|||
Thickness | 88.9 microns | 3.50 mil | side 1 silicone; Arlon SQA-TMS-003 |
Arlon 51141R015 Silicone Rubber/Fiberglass Laminate Interleave 1: 3 mil PE; Side 1: uncured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave 2: 3 mil PE |
|||
Thickness | 88.9 microns | 3.50 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 51571B015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical.. |
|||
Thickness | >= 88.9 microns | >= 3.50 mil | Side 2 |
Arlon 51571XC015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 88.9 microns | 3.50 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51576R015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mate.. |
|||
Thickness | 88.9 microns | 3.50 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 51576XC015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Cured Silicone Rubber This data represents typical values for the production mat.. |
|||
Thickness | 88.9 microns | 3.50 mil | Side 2, Layer 2; Arlon SQA-TMS-003 |
Arlon 51588R019 0.019" (0.483 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2, Layer 1: Cured Silicone RubberSide 2, Layer 2: Uncured Silicone Rubber Interleave: Polyethylene Appearanc.. |
|||
Thickness | >= 88.9 microns | >= 3.50 mil | Side 1 |
Arlon 51601W015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberProduct Use: Flexible heater insulationAppearance: White silicone gum on fiberglass with polymer release linersThis .. |
|||
Thickness | 88.9 microns | 3.50 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 51866R015 0.0170" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Thickness | 88.9 microns | 3.50 mil | Tape |
3M 9737 Double Coated Splicing Tape 3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrierFeatures:High tack, acrylic adhesive offers good low and elevated temperature resistance.Adheres.. |
|||
Thickness | 88.9 microns | 3.50 mil | Release Liner |
3M ATG 987 Tape 3M™ ATG Adhesive Transfer Tape 987 is a 1.7 mil, 400 acrylic, reverse wound, pressure sensitive adhesive on a densified kraft paper liner. Utility grade tape. For use with Scotch® ATG Adhesive App.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV031 Indoor UL Recognized White Vinyl Label Products 3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV1222R Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are soft white vinyl label stocks that offer durability and good conformability. These vinyl labels utilize 3M™ Adhesive R3500, which is designed for use on smoo.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV362 Soft Yellow Vinyl Label Products 3M™ Soft Yellow Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clar.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV517 Semi-Rigid Vinyl Label Product 3M™ Semi-Rigid Vinyl Label Products are semi-rigid white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1410, which is a general purpose.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FVT36 Tire Label Product 3M™ Tire Label Products utilize a flexible and conformable white vinyl labelstock that offers durability, moisture resistance, and dimensional stability. 3M™ Adhesive G1120, a rubber-based aggress.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FVT44 Tire Label Product 3M™ Tire Label Products utilize a flexible and conformable white vinyl labelstock that offers durability, moisture resistance, and dimensional stability. 3M™ Adhesive G1120, a rubber-based aggress.. |
|||
Thickness | 88.9 microns | 3.50 mil | Liner; ASTM D3752 |
3M 5423 Polyethylene Tape 3M™ Polyethylene Tape 5422 has a rubber adhesive which provides an excellent abrasion resistant surface.Information provided by 3M |
|||
Thickness | >= 88.9 microns | >= 3.50 mil | Side 1 |
Arlon R33991R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | >= 88.9 microns | >= 3.50 mil | Side 2 |
Arlon R33991R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV023205 White Vinyl Label Products 3M™ White Vinyl Label Products are flexible and conformable materials that offer durability and moisture resistance. The polymerically plasticized nature of this soft vinyl imparts long term dimens.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV030 Indoor UL Recognized White Vinyl Label Products 3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV032 Indoor UL Recognized White Vinyl Label Products 3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,.. |
|||
Thickness | 88.9 microns | 3.50 mil | Release Liner |
3M 450XL Extended Liner Tapes 3M™ Extended Liner Tapes have a liner that extends beyond the width of the adhesive to provide easy liner starting and removal. The liners, with the exception of 3M™ Extended Liner Tape 450EK is p.. |
|||
Thickness | 88.9 microns | 3.50 mil | Adhesive |
3M 9653LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Thickness | 88.9 microns | 3.50 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 48981R010 0.0100" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: 3 mil PolyethyleneSide 1: Uncured RubberSubstrate: Style 1080 FiberglassSide 2: Uncured Silicone RubberInterleave 2: 3 mil PolyethyleneThis data represents typic.. |
|||
Thickness | 88.9 microns | 3.50 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 48981R010 0.0100" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: 3 mil PolyethyleneSide 1: Uncured RubberSubstrate: Style 1080 FiberglassSide 2: Uncured Silicone RubberInterleave 2: 3 mil PolyethyleneThis data represents typic.. |