Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 813 microns | 32.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 19563R032 0.032" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1523 FiberglassSide 2: Cured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the producti.. |
|||
Thickness | 813 microns | 32.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55578XA030 0.032" (0.813 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: 162 Style Fiberglass Side 1: Cured Silicone Rubber (Skim Coat).. |
|||
Thickness | 813 - 914 microns | 32.0 - 36.0 mil | Overall |
Arlon 55579R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured layer on top of a cured layer on one side Appearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production materi.. |
|||
Thickness | 813 microns | 32.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 31140R025 0.032" Uncured Silicone Rubber on Release Coated HDPE Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberRelease Carrier: Release Coated HDPEThis data represents typical values for the production material and should no.. |
|||
Thickness | 813 microns | 32.0 mil | overall; Arlon SQA-TMS-003 |
Arlon 53423R032 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 2523 fiberglass; Side 2: cured silicone rubber |
|||
Thickness | 813 microns | 32.0 mil | Prime Coated 3784 Fiberglass, Substrate |
Arlon 59463X068CT 0.068" (1.73 mm) Textured, Cured Rubber with Fiberglass Substrate Design/Construction:Side 1: Textured, Cured Rubber Side 2: Textured, Cured Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 813 microns | 32.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R30342R032 0.032" (0.813 mm) Cured Silicone Rubber Design/Construction:Product: Cured Silicone Rubber Liner: PolyethyleneAppearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used to w.. |