Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-012 |
Arlon A1030-R008-12 0.030" (0.762 mm) Fully Cured Fusible Silicone Rubber - Extruded Fusible Tape
(disco 2 inches width and 36 inches long. Design/Construction: Interleave: Polyester Film Extruded Fusible Tape (Rectangular Cross Section): Fully Cured Fusible Silicone RubberThis data represents typical.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-012 |
Arlon A1030-X008-12 0.030" (0.762 mm) Fully Cured Fusible Silicone Rubber - Extruded Fusible Tape
(disco 1 inch width and 36 inches long. Design/Construction: Interleave: Polyester Film Extruded Fusible Tape (Rectangular Cross Section): Fully Cured Fusible Silicone RubberThis data represents typical v.. |
|||
Thickness | 762 microns | 30.0 mil | Silicone |
Arlon 41400R030 0.030" Uncured, Unsupported Silicone Rubber on a Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 49481R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1681 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical .. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55572R030 0.030" (0.762 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. T.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55576R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Uncured Silicone Rubber Interleave: LDPE This data represents typical values for the production material. T.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55590R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. The data should not be us.. |
|||
Thickness | 762 - 838 microns | 30.0 - 33.0 mil | Overall |
Arlon 55596R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55638R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater SubstrateAppearance: Red silic.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 930-10Bxx-P0 0.030" (0.762 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 30 mil thick, Black, Rectangular cross-section, Self-fu.. |
|||
Thickness | 762 microns | 30.0 mil | Rubber; Arlon SQA-TMS-012 |
Arlon 930-10Rxx-P1 0.030" Self-Fusing Silicone Rubber Tape 1 inch wide, 30 mil thick, red, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.Desi.. |
|||
Thickness | 762 microns | 30.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon HSLW301R##-P0 0.030" (0.762 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: High Strength, 1 inch wide, 30 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicate.. |
|||
Thickness | 762 microns | 30.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon LW3015B##-P0 0.030" (0.762 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1.5 inch wide, 30 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll leng.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R30711R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1165 Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: PolyethyleneAppearance: Red silicone gum .. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R30960T030 0.030" (0.762 mm) Uncured Silicone Rubber with Kodacel Substrate Design/Construction:Interleave: PolyethyleneAdd-on: Uncured Silicone Rubber Substrate: Kodacel CarrierAppearance: Translucent, high viscosity gum on release linersThis data represents typical values.. |
|||
Thickness | 762 microns | 30.0 mil | |
3M Scotch® 77 Black Fire-Retardant Electric Arc Proofing Tape Scotch® Fire-Retardant Electric Arc Proofing Tape 77 Series are designed to protect most types of electrical cables from fault arc-generated heat and flames of nearby cable failures. These elastome.. |
|||
Thickness | 762 microns | 30.0 mil | |
3M Scotch™ 130C Linerless Rubber Splicing Tape 3M™ Scotch™ Linerless Rubber Splicing Tape 130C is a high conformable, linerless, ethylene rubber (EPR), high-voltage insulating tape, formulated to provide excellent thermal dissipation of splice.. |
|||
Thickness | 762 microns | 30.0 mil | |
3M Scotch™ 23 Rubber Splicing Tape Scotch® Rubber Splicing Tape 23 is a highly conformable, self-fusing EPR (Ethylene Propylene Rubber) based, high voltage splicing tape. It is a non-vulcanizing, shelf-stable tape with excellent ele.. |
|||
Thickness | 762 microns | 30.0 mil | Silicone |
Arlon 41580B030 0.030" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Thickness | 762 microns | 30.0 mil | Silicone |
Arlon 41580R030 0.030" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 51946C030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 1: Cured Silicone Wash Coat Appearance: Brown silicone rubber and gum on fiberglass.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55100R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass fabricT.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55106R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silic.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55108R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2, Layer 2: Uncured Silicone RubberSide 2, Layer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone Rubber This data rep.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55146R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red sili.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R38081R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassSide 2: Uncured SiliconeInterleave 2: Polyethylene This data represents typical values .. |
|||
Thickness | 762 microns | 30.0 mil | |
3M Temflex™ 2155 Rubber Splicing Tape Temflex 2155 Rubber Splicing Tape is a conformable self-fusing rubber electrical insulating tape. It is designed for low voltage electrical insulating and moisture sealing applications. Temflex 2155.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 44141R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Clear PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Blue PolyethyleneThis data represent.. |
|||
Thickness | 762 microns | 30.0 mil | Rubber; Arlon SQA-TMS-012 |
Arlon T2030-R004-12 0.030" Cured Self-Fusing Silicone Rubber Tape 1 inch wide, 30 mil thick, 12.0 yards long, red, triangular cross-section, self-fusing silicone tape.Design/Construction:Interleave: 1 mil PETProduct: Cured Silicone Self-fusing RubberCross-section.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55276R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Cured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silic.. |