Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 610 microns | 24.0 mil | |
Fibre Glast 660 6K, 5HS Weave Carbon Fiber Fabric Graphite fibers contain up to 95% carbon and yield the highest tensile strength in the FRP industry. These fibers woven together form graphite fabric. These fabrics offer higher strength and stiffne.. |
|||
Thickness | 610 microns | 24.0 mil | Standard; Laminate |
GrafTech GRAFOIL® GHH Standard Internal Combustion Laminate, Metal Reinforced GRAFOIL® Grade GHH is a laminate made with GRAFOIL® Grade GTC flexible graphite chemically bonded to both faces of a flat, low-carbon steel core. Its applications include: exhaust sealing, ga.. |
|||
Thickness | 610 microns | 24.0 mil | Nominal |
DuPont™ Nomex® 410 Paper, 24 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Thickness | 610 microns | 24.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 51576R024A 0.024" (0.610 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
Thickness | >= 610 microns | >= 24.0 mil | Side 2 |
Arlon 51586R035 0.035" (0.889 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mate.. |
|||
Thickness | 610 microns | 24.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55142R040 0.040" (1.02 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass This data represents typical values for the production material. The data should not be use.. |
|||
Thickness | 610 microns | 24.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55572AA024 0.024" (0.610 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass This data represents typical values for the production material. The data should not be us.. |
|||
Thickness | 610 - 711 microns | 24.0 - 28.0 mil | Overall |
Arlon 56590R026 0.026" (0.660 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis data Represents typical values fo.. |
|||
Thickness | 610 - 711 microns | 24.0 - 28.0 mil | Overall |
Arlon 56606R026M 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass with polymer release li.. |
|||
Thickness | 610 - 660 microns | 24.0 - 26.0 mil | Overall |
Arlon P29609R025 0.025" (0.635 mm) Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Layer-on-Layer Product Use: Traction motor insulation, electrical insulationAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the pr.. |
|||
Thickness | 610 - 711 microns | 24.0 - 28.0 mil | Overall |
Arlon R34696R026 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 610 microns | 24.0 mil | Side 2 add-on thickness; Arlon SQA-TMS-003 |
Arlon R39118R037L 0.037" (0.940 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyester Release Liner Transfer Pressure Sensitive Adhesive: Silicone PSASide 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Cured Silicone Rubber.. |
|||
Thickness | 610 microns | 24.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 55102R024 0.024" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production material and should not be used as material specifications.In.. |
|||
Thickness | 610 microns | 24.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55272R024 0.024" (0.610 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. The data should not be use.. |
|||
Thickness | 610 - 711 microns | 24.0 - 28.0 mil | Overall |
Arlon R33706R026 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass with polymer release li.. |