Physical Properties Metric English Comments
Thickness 533 - 991 microns
21.0 - 39.0 mil
Range of Thicknesses Available
Rogers Corporation Poron® 4701-15 Urethane Foam, Soft Seal
PORON® 4701-15 Improved Soft Seal SeriesEnhanced Surface Toughness, Reliable Materials for Thinner DesignsIncreased Surface Toughness, Improved YieldsExcellent Compressibility and ConformabilityLon..
Thickness 533 - 991 microns
21.0 - 39.0 mil
Range of Thicknesses Available
Rogers Corporation Poron® Shock Seal™ 4790-79-12 Handheld Urethane Foam, Handheld Grade, PET Reinforced
Extreme Impact Protection, Ultimate ReliabilitySpecifically engineered to protect sensitive components from damage caused by impactConsistent cushioning performance through repeated impactsExcellent..
Thickness 533 - 991 microns
21.0 - 39.0 mil
Range of Thicknesses Available
Rogers Corporation Poron® Shock Seal™ 4790-79-9 Handheld Urethane Foam, Handheld Grade, PET Reinforced
Extreme Impact Protection, Ultimate ReliabilitySpecifically engineered to protect sensitive components from damage caused by impactConsistent cushioning performance through repeated impactsExcellent..
Thickness 533 microns
21.0 mil
nominal, cured, per ply
Park Electrochemical Nelcote® F-554 Phenolic Prepreg, Aerospace Silica Fabric Reinforced
Nelcote® F-554 is a high purity silica filled phenolic resin coated on Commercial or Aerospace grade silica fabric. F-554 is used in the manufacture of intermediate temperature ablative rocket nozz..
Thickness 533 microns
21.0 mil
nominal, cured, per ply
Park Electrochemical Nelcote® F-554 Phenolic Prepreg, Commercial Silica Fabric Reinforced
Nelcote® F-554 is a high purity silica filled phenolic resin coated on Commercial or Aerospace grade silica fabric. F-554 is used in the manufacture of intermediate temperature ablative rocket nozz..
Thickness 533 microns
21.0 mil
nominal, cured, per ply
Park Electrochemical Nelcote® F-557 Phenolic Prepreg, Aerospace Silica Fabric Reinforced
Nelcote® F-557 is a high purity silica filler phonic resin coated on Commercial or Aerospace grade silica fabric. F-557 is used in the manufacture of intermediate temperature ablative rocket nozzle..
Thickness 533 microns
21.0 mil
nominal, cured, per ply
Park Electrochemical Nelcote® F-557 Phenolic Prepreg, Commercial Silica Fabric Reinforced
Nelcote® F-557 is a high purity silica filler phonic resin coated on Commercial or Aerospace grade silica fabric. F-557 is used in the manufacture of intermediate temperature ablative rocket nozzle..
Thickness 533 - 1190 microns
21.0 - 47.0 mil
Range of Thicknesses Available
Rogers Corporation Poron® 4701-30-25 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which enab..
Thickness 533 - 1040 microns
21.0 - 41.0 mil
Range of Thicknesses Available
Rogers Corporation Poron® 4790-92-25 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
Thickness >= 533 microns
>= 21.0 mil
Side 1
Arlon 55531R060 0.061" (1.55 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. Th..
Thickness >= 533 microns
>= 21.0 mil
Side 2
Arlon 55531R060 0.061" (1.55 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. Th..
Thickness >= 533 microns
>= 21.0 mil
Side 1, Uncured Rubber Layer
Arlon 55579R043W 0.043" (1.09 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured layer on top of a cured layer on one side This data Represents typical values for the production material. The data should not be used to write, or in place of, m..
Thickness 533 microns
21.0 mil
Side 2
Arlon R35121R063 0.063" (1.60 mm) Uncured Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured RubberSide 2: Uncured Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material speci..
Thickness 533 - 584 microns
21.0 - 23.0 mil
3M Panagraphics™ III Wide Width Flexible Substrate
22 mil white-pigmented vinyl substrate with a polyester scrim; Smooth front surface with a semi-gloss finish; Decorate first or second surface with inkjet direct printing or first surface with cut f..
Thickness 533 microns
21.0 mil
side 1; Arlon SQA-TMS-003
Arlon 55143R060 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 2: cured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber
Thickness 533 microns
21.0 mil
side 2; Arlon SQA-TMS-003
Arlon 55143R060 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 2: cured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber
Thickness 533 microns
21.0 mil
Side 1; Arlon SQA-TMS-003
Arlon 55273R060 0.060" (1.52 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, ..
Thickness 533 microns
21.0 mil
Side 2; Arlon SQA-TMS-003
Arlon 55273R060 0.060" (1.52 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, ..
Copyright © lookpolymers.com All Rights Reserved