Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 51.0 microns | 2.01 mil | |
Parker Chomerics WIN-SHIELD™ F Conductive Film Information provided by Chomerics |
|||
Thickness | 51.0 microns | 2.01 mil | |
NOVA Chemicals Sclair® FP112-A Octene VLDPE Film Resin Features: Low seal initiation temperatureHigh toughnessVery good optical propertiesComplies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Low gel Applications: Sealant and lamination film for food packagi.. |
|||
Thickness | 51.0 microns | 2.01 mil | Standard |
GrafTech eGRAF® SPREADERSHIELD™ SS400 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Thickness | 51.0 microns | 2.01 mil | |
Dow AFFINITY™ FM 1570 Polyolefin Plastomer AFFINITY® FM 1570 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide film products with excellent sealability and high hot tack strength, outstanding blown film optics, and .. |
|||
Thickness | 51.0 microns | 2.01 mil | |
Dow AFFINITY™ PF 1140 Polyolefin Plastomer AFFINITY® PF 1140 polyolefin plastomer is an ethylene alpha-olefin resin designed for use in a variety of demanding applications including high-speed, form-fill seal products, display films and fre.. |
|||
Thickness | 51.0 microns | 2.01 mil | |
Dow AFFINITY™ PL 1880 Polyolefin Plastomer AFFINITY® PL 1880 polyolefin plastomer is an ethylene alpha-olefin resin designed for use in a variety of demanding packaging applications including high-speed, form-fill seal products. AFFINITY PL.. |
|||
Thickness | 51.0 microns | 2.01 mil | |
Dow ATTANE™ 4213 Ultra Low Density Polyethylene ATTANE® 4213 copolymer is an ultra low density polyethylene that offers excellent flexibility, sealability, puncture resistance and superior strength. It exhibits oxygen transmission characteristic.. |
|||
Thickness | 51.0 microns | 2.01 mil | Film (Backing) Thickness |
Caplinq LINQTAPE™ PIT2A Product Description: LINQTAPE™ PIT-Series is a high-temperature resistant polyimide tape designed for both permanent and temporary bonding in many high temperature applications. Additionally, it p.. |
|||
Thickness | 51.0 microns | 2.01 mil | Film (Backing) Thickness |
Caplinq LINQTAPE™ PIT2S Product Description: LINQTAPE™ PIT-Series is a high-temperature resistant polyimide tape designed for both permanent and temporary bonding in many high temperature applications. Additionally, it p.. |