Polymer Property : Thickness = 216 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 216 microns
8.50 mil
Hexcel® HexForce™ 1581 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Thickness 216 microns
8.50 mil
Hexcel® HexForce™ 7635 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Thickness 216 microns
8.50 mil
ASTM D645
3M 6147 Performance Reinforced Water Activated Tape
3M™ Performance Reinforced Water Activated Tape 6147 is used for box sealing and other packaging applications. This has a fiberglass reinforced paper backing and a high tack water activated adhesiv..
Thickness 216 microns
8.50 mil
Side 2 Layer 2; Arlon SQA-TMS-003
Arlon 55578GA028 0.0280" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: LDPESide 2 Layer 2: Uncured Silicone RubberSide 2 Layer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents ty..
Thickness 216 microns
8.50 mil
Side 2 Layer 2; Arlon SQA-TMS-003
Arlon 55578XA028 0.0280" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: LDPESide 2 Layer 2: Uncured Silicone RubberSide 2 Layer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents ty..
Thickness 216 microns
8.50 mil
Side 1; Arlon SQA-TMS-003
Arlon P29514R015 0.0165" (0.419 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassProduct Advatages:Flexibility: Silicone rubber resists damage due to vibration, frame movement under loa..
Thickness 216 microns
8.50 mil
Overall thickness
Arlon R33073X0085 0.0085" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: 7628 FiberglassSide 2: Cured Silicone RubberInterleave: NoneThis data represents typical values for the production material and should ..
Thickness 216 microns
8.50 mil
Overall; Arlon SQA-TMS-003
Arlon 44576R009A 0.0058" (0.216 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 1165 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production ma..
Thickness 216 - 267 microns
8.50 - 10.5 mil
Overall
Arlon 47576R009 0.0095" (0.241 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured RubberSide 2: Uncured RubberAppearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production material. The data sho..
Thickness 216 microns
8.50 mil
Overall Thickness
Arlon 51163X0085 0.0085" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone Rubber50" wideThis data represents typical values for the production material and should not..
Thickness 216 microns
8.50 mil
3M Scotch® Super 88 Vinyl Electrical Tape
Scotch® Vinyl Electrical Tape Super 88 is a premium grade, 8.5 mil thick, all-weather vinyl-insulating tape. It is designed to perform continuously in ambient temperatures up to 105°C. The tape is..
Thickness 216 - 241 microns
8.50 - 9.50 mil
Adhesive and protective top covering
3M 3635-100 Light Enhancement Film
A light box or channel letter contains lighting elements that illuminate the front sign face and transmit some light to the viewer. However much of the illumination is reflected or absorbed by other..
Thickness 216 microns
8.50 mil
Layer 2; Arlon SQA-TMS-003
Arlon 55279R031 0.031" (0.787 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s..