Polymer Property : Thickness = 211 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 211 microns
8.30 mil
Total Thickness
3M 9088FL High Performance Double Coated Tapes with Adhesive 375
3M™ Double Coated Tapes with 3M™ Adhesive 375 provides a high level of adhesive peel and shear performance. The adhesive system used on these products provides good adhesion to both high and low s..
Thickness 211 microns
8.30 mil
Substrate; Arlon SQA-TMS-003
Arlon UltraPad™ 51073G031D Silicone-Based Press Pad
Green UltraPad™ D65: Silicone Based Press PadDesign/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberThis data..
Thickness 211 microns
8.30 mil
Substrate; Arlon SQA-TMS-003
Arlon UltraPad™ 51073R031D Silicone-Based Press Pad
UltraPad™ D65: Silicone Based Press PadDesign/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberThis data repre..
Thickness 211 microns
8.30 mil
Substrate; Arlon SQA-TMS-003
Arlon UltraPad™ 55073R031 Silicone-Based Press Pad
UltraPad™ D65: Silicone Based Press PadDesign/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberThis data repre..
Thickness 211 microns
8.30 mil
Liner; ASTM D3752
3M 365 Thermosetable Glass Cloth Tape
3M™ Glass Cloth Tape 365 is a thermosetable rubber-resin adhesive tapes coated onto a strong conformable glass backing for many applications requiring high adhesion for adhesion to a variety of sur..
Thickness 211 microns
8.30 mil
Liner; ASTM D3752
3M 3650 Thermosetable Glass Cloth Tape
3M™ Glass Cloth Tape 3650 is a thermosetable rubber-resin adhesive tapes coated onto a strong conformable glass backing for many applications requiring high adhesion for adhesion to a variety of su..
Thickness 211 microns
8.30 mil
Total Thickness
3M 9088 High Performance Double Coated Tapes with Adhesive 375
3M™ Double Coated Tapes with 3M™ Adhesive 375 provides a high level of adhesive peel and shear performance. The adhesive system used on these products provides good adhesion to both high and low s..