Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 2030 - 9530 microns | 80.0 - 375 mil | Range of Thicknesses Available |
Rogers Corporation Poron® Shock Seal™ 4790-79-12 Urethane Foam, Industrial Grade Thickness: 0.080"- 0.375"Color: BlackInformation provided by Rogers Corporation. |
|||
Thickness | 2030 microns | 80.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 10502N080 0.080" (2.3 mm) Cured Silicone Rubber (Unsupported)
(discontinued **) Vacuum Bag SubstrateDesign/Construction:Interleave: PolyethyleneMaterial: Cured Silicone RubberAppearance: Translucent silicone rubberThis data represents typical values for the production material... |
|||
Thickness | 2030 microns | 79.9 mil | |
GrafTech GRAFOIL® GHC Standard Internal Combustion Laminate GRAFOIL® Grade GHC is a laminate made from Grade GTC flexible graphite. Laminate Construction: GRAFOIL® Grade GTC ? Micro-thin, phenolic-based adhesive ? GRAFOIL® Grade GTC |
|||
Thickness | 2030 microns | 80.0 mil | Total |
3M 4412G Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Thickness | 2030 microns | 80.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 10172R080 0.080" (2.3 mm) Cured Silicone Rubber Vacuum Bag Reversion Resistant Vacuum Bag SubstrateDesign/Construction:Interleave: PolyethyleneMaterial: Cured Silicone RubberAppearance: Red silicone rubberThis data represents typical values for the producti.. |
|||
Thickness | 2030 microns | 80.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 680-R3839R 0.084" (2.13 mm) Cured Silicone Coating with Silica-based Substrate Design/Construction:Side 1: Cured Silicone Coating Substrate: Silica-basedSide 2: Cured Silicone Coating Rubber Application Advantages:Extremely low thermal conductivityThermally stableBondable to s.. |
|||
Thickness | 2030 microns | 80.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 680-R3844R 0.084" (2.13 mm) Cured Silicone Coating with Silica-based Substrate Design/Construction:Side 1: Cured Silicone Coating Substrate: Silica-basedSide 2: Cured Silicone Coating Rubber Application Advantages:Extremely low thermal conductivityThermally stableBondable to s.. |
|||
Thickness | 2030 microns | 80.0 mil | Total |
3M 4412N Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |