Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 18.0 - 50.0 microns | 0.709 - 1.97 mil | Recommended |
Polimeri Europa Riblene® FM 34 Low Density Polyethylene - Blown Film Extrusion Riblene FM 34 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 is characterized by a good balance between processabilit.. |
|||
Thickness | 18.0 - 50.0 microns | 0.709 - 1.97 mil | Recommended |
Polimeri Europa Riblene® FM 50 Low Density Polyethylene - Blown Film Extrusion Riblene FM 50 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FM 50 is characterized by optimum optical properties and rigidity.Films manufactured with Riblene FM 50.. |
|||
Thickness | 18.0 - 50.0 microns | 0.709 - 1.97 mil | Recommended |
Polimeri Europa Riblene® FM 53 Low Density Polyethylene - Blown Film Extrusion Riblene FM 53 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 53 is characterized by optimum optical properties and rigid.. |
|||
Thickness | 18.0 - 50.0 microns | 0.709 - 1.97 mil | Recommended |
Polimeri Europa Riblene® FM 34 E Low Density Polyethylene - Blown Film Extrusion Riblene FM 34 E is a low density polyethylene (LDPE) with added slip (erucamide) and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 E is characterized by a good balance betwe.. |
|||
Thickness | 18.0 microns | 0.709 mil | ± 3.0%; ASTM-252-78 |
Kinlead HSD11 Normal Grade Heat Sealable Film (thickness: 18 µm) HSD11 is a general, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dim.. |
|||
Thickness | 18.0 microns | 0.709 mil | ± 3.0%; ASTM-252-78 |
Kinlead HSD12 Normal Grade Heat Sealable Film (thickness: 18 µm) HSD12 is a printing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona trea.. |
|||
Thickness | 18.0 microns | 0.709 mil | ± 3.0%; ASTM-252-78 |
Kinlead HSS11 Normal Grade Heat Sealable Film (thickness: 18 µm) HSS11 is a general, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dimens.. |
|||
Thickness | 18.0 microns | 0.709 mil | ± 3.0%; ASTM-252-78 |
Kinlead HSS12 Normal Grade Heat Sealable Film (thickness: 18 µm) HSS12 is a printing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona treatme.. |
|||
Thickness | 18.0 microns | 0.709 mil | ± 3.0%; ASTM-252-78 |
Kinlead HSS13 Normal Grade Heat Sealable Film (thickness: 18 µm) HSS13 is a metalizing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has coron.. |
|||
Thickness | 18.0 microns | 0.709 mil | ± 3.0%; ASTM-252-78 |
Kinlead LSD11 Low Temperature Grade Heat Sealable Film (thickness: 18 µm) LSD11 is a general, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has co.. |
|||
Thickness | 18.0 microns | 0.709 mil | ± 3.0%; ASTM-252-78 |
Kinlead LSD12 Low Temperature Grade Heat Sealable Film (thickness: 18 µm) LSD12 is a printing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has co.. |
|||
Thickness | 18.0 microns | 0.709 mil | ± 3.0%; ASTM-252-78 |
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 18 µm) LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron.. |
|||
Thickness | 18.0 microns | 0.709 mil | ± 3.0%; ASTM-252-78 |
Kinlead LSS12 Low Temperature Grade Heat Sealable Film (thickness: 18 µm) LSS12 is a printing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has coron.. |
|||
Thickness | 18.0 microns | 0.709 mil | ± 3.0%; ASTM-252-78 |
Kinlead ML11 General Grade BOPP Matt Film (thickness: 18 µm) ML11 is a general grade BOPP Matt film. It is translucent and non heat sealable. It has low static and a good matt surface. One side has corona treatment. It is specially designed for board laminati.. |
|||
Thickness | 18.0 microns | 0.709 mil | ± 3.0%; ASTM-252-78 |
Kinlead PL11 Lamination Grade BOPP Plain Film (thickness: 18 µm) PL11 is a general, lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. One side has corona treatment. It is widely used in laminating.. |
|||
Thickness | 18.0 microns | 0.709 mil | ± 3.0%; ASTM-252-78 |
Kinlead PL13 Lamination Grade BOPP Plain Film (thickness: 18 µm) PL13 is a woven bag lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. One side has corona treatment. It is widely used in laminatin.. |
|||
Thickness | 18.0 microns | 0.709 mil | ± 3.0%; ASTM-252-78 |
Kinlead PL21 Lamination Grade BOPP Plain Film (thickness: 18 µm) PL21 is a general, lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. It has excellent dimensional stability, high tensile strength,.. |
|||
Thickness | 18.0 microns | 0.709 mil | ± 3.0%; ASTM-252-78 |
Kinlead PM11 Metalizing Grade BOPP Plain Film (thickness: 18 µm) PM11 is a general, metalizing grade BOPP plain film. It is transparent and non heat sealable. It has good heat resistance and tensile strength, and it has excellent metal adhesion. One side has coro.. |
|||
Thickness | 18.0 microns | 0.709 mil | ± 3.0%; ASTM-252-78 |
Kinlead PP11 Printing Grade BOPP Plain Film (thickness: 18 µm) PP11 is a general, printing grade BOPP plain film. It is transparent and non heat sealable. It has excellent ink adhesion. One side has corona treatment. It is widely used in printing applications.I.. |
|||
Thickness | 18.0 - 25.0 microns | 0.709 - 0.984 mil | |
Gwent Electronic Materials C2050503D1 Curable Carbon Ink This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive coating that combines good adhesion with excellent chemical, solvent and .. |
|||
Thickness | 18.0 microns | 0.709 mil | Cured, Typical, Using a 230 mesh stainless steel screen, 13 micron emulsion |
Gwent Electronic Materials C2051014P10 Silver/Silver Chloride Paste Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 70/30. Applications in medical diagnostics, environmentalScreen Printing Equipment: semi-automatic, manualScreen Types: polye.. |
|||
Thickness | 18.0 microns | 0.709 mil | Cured, Typical, Using a 230 mesh stainless steel screen, 13 micron emulsion |
Gwent Electronic Materials C2080110D2 Silver/Silver Chloride Paste Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 70/30. This is has been designed for fine line printing.Screen Printing Equipment: semi-automatic, manualScreen Types: polye.. |
|||
Thickness | 18.0 microns | 0.710 mil | ExxonMobil Method |
ExxonMobil Metallyte™ 18MM348 OPP Film Product Description: An enhanced barrier metalized film with a very broad seal range designed to be used in laminate with OPP or Polyester for HFFS applications. The design of this film allows excel.. |
|||
Thickness | 18.0 microns | 0.710 mil | ExxonMobil Method |
ExxonMobil Metallyte™ 18MM383 OPP Film Product Description: A biaxially oriented very high barrier metalized polypropylene film. This film offers an outstanding moisture barrier and a broad seal range surface on the other side. This film.. |
|||
Thickness | 18.0 microns | 0.710 mil | ExxonMobil Method |
ExxonMobil Metallyte™ 18MM388 OPP Film Product Description: A metallized biaxially oriented polypropylene film, metalized on one side with a broad seal range surface on the other side. This film is designed for high barrier performance p.. |
|||
Thickness | 18.0 microns | 0.710 mil | ExxonMobil Method |
ExxonMobil Metallyte™ 18MM483 OPP Film Product Description: A biaxially oriented polypropylene film, metalized on one side with a broad seal range surface on the other side. This film is designed for high barrier performance packaging ap.. |
|||
Thickness | 18.0 microns | 0.710 mil | ExxonMobil Method |
ExxonMobil Metallyte™ 18MM488 OPP Film Product Description: A metalized biaxially oriented polypropylene film, metalized on one side. MM488 is typically used in laminates as the inner web for VFFS and HFFS applications. Due to its slip c.. |
|||
Thickness | 18.0 microns | 0.710 mil | ExxonMobil Method |
ExxonMobil Metallyte™ 18MM882 OPP Film Product Description: An ultra high barrier (UHB), biaxially oriented, multilayer polypropylene film. In addition to an excellent water vapor barrier, this film has an exceptional barrier to oxygen, .. |
|||
Thickness | 18.0 microns | 0.710 mil | ExxonMobil Method |
ExxonMobil Metallyte™ 18MM883 OPP Film Product Description: An ultra high barrier (UHB), biaxially oriented multilayer polypropylene film. This film has an exceptional barrier to oxygen, flavors and aromas and has an excellent water vapo.. |
|||
Thickness | 18.0 microns | 0.709 mil | Critical Film Thickness; AGFP Method |
Asahi Glass Fluon® XAD938 PTFE Aqueous Dispersion Fluon®PTFE aqueous dispersions are useful for glass cloth coating, metal coating, binder, additive in resin, feedstock of heat resistive paint ,etc.Information provided by Asahi Glass Company, Inc... |