Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 17.0 microns | 0.669 mil | extruded at 4:1 BUR |
Lotte Chemical Titan TITANEX® HF0961 High density polyethylene Hexene-1 resin HF0961 is a pelleted high molecular weight, high density polyethylene Hexene-1 resin for tubular film extrusion.Applications: Grocery sacks, shopping bags, liners notion and millinery bags.Advantag.. |
|||
Thickness | 17.0 microns | 0.669 mil | extruded at 4:1 BUR |
Lotte Chemical Titan TITANZEX® HF7000 High density polyethylene HF7000 is a high density polyethylene resin for tubular film extrusion. HF7000 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1.. |
|||
Thickness | 17.0 microns | 0.669 mil | extruded at 4:1 BUR |
Lotte Chemical Titan TITANZEX® HF7700 High density polyethylene HF7700 is a high density polyethylene resin for tubular film extrusion. HF7700 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1.. |
|||
Thickness | 17.0 microns | 0.669 mil | when printed through a 156 mesh |
Gwent Electronic Materials C2000215D3 Silver / Silver Chloride Paste C2000215D3 has a ratio of Silver to Silver Chloride of 80/20. This is used for reference electrodes in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries. It forms part of a .. |
|||
Thickness | 17.0 microns | 0.669 mil | Using a 156 mesh stainless steel screen, 13 micron emulsion |
Gwent Electronic Materials C2000218D5 Silver/Silver Chloride Paste Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 90/10. It is specifically designed to give good adhesion to ceramic substrates. Applications in medical diagnostics, environm.. |
|||
Thickness | 17.0 microns | 0.669 mil | when printed through a 156 mesh |
Gwent Electronic Materials C60531D1 Silver / Silver Chloride Paste C60531D1 has a ratio of Silver to Silver Chloride of 90/10. This is used for reference electrodes in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries. It forms part of a fa.. |
|||
Thickness | 17.0 microns | 0.669 mil | extruded at 4:1 BUR |
Lotte Chemical Titan TITANEX® HF1881 High density polyethylene Hexene-1 resin HF1881 is a pelleted medium molecular weight, high density polyethylene Hexene-1 resin for tubular film extrusion.Applications: Grocery sacks, shopping bags, liners and thin films.Advantages: Speci.. |
|||
Thickness | 17.0 microns | 0.670 mil | ExxonMobil Method |
ExxonMobil Label-Lyte™ 17LL222 OPP Film Product Description: An uncoated biaxially oriented, transparent polypropylene film designed for overlamination in labeling applications where high gloss and high transparency are required.Availabil.. |
|||
Thickness | 17.0 microns | 0.670 mil | ExxonMobil Method |
ExxonMobil Bicor™ 17MB400 OPP Film Product Description: Bicor 17MB400 is one side treated, sealable coextruded OPP film. It is designed for use in laminations.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features:Ou.. |