Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 152 microns | 6.00 mil | cured, per ply |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T700 Uni Tape Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Thickness | 152 microns | 6.00 mil | side 1; Arlon SQA-TMS-003 |
Arlon A3020-T002-12 Silicone Rubber/Fiberglass Laminate
(discontinued **) Side 1: cured fusible silicone rubber; Substrate: 25% sinusoidal fiberglass; Side 2: cured fusible silicone rubber; Interleave: 1 mil PE film |
|||
Thickness | 152 microns | 6.00 mil | side 1; Arlon SQA-TMS-003 |
Arlon A3020-T004-12 Silicone Rubber/Fiberglass Laminate
(discontinued **) Side 1: cured fusible silicone rubber; Substrate: 25% sinusoidal fiberglass; Side 2: cured fusible silicone rubber; Interleave: 1 mil PE film |
|||
Thickness | 152 microns | 6.00 mil | side 2; Arlon SQA-TMS-003 |
Arlon A3020-T004-12 Silicone Rubber/Fiberglass Laminate
(discontinued **) Side 1: cured fusible silicone rubber; Substrate: 25% sinusoidal fiberglass; Side 2: cured fusible silicone rubber; Interleave: 1 mil PE film |
|||
Thickness | >= 152 microns | >= 6.00 mil | Side 1 |
Arlon 518581R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. Th.. |
|||
Thickness | >= 152 microns | >= 6.00 mil | Side 2 |
Arlon 518581R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. Th.. |
|||
Thickness | 152 microns | 6.00 mil | Layer 2; Arlon SQA-TMS-003 |
Arlon 18609R023 0.023" (0.584 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: PolyethyleneLayer 1: Cured Silicone RubberLayer 2: Uncured Silicone RubberSubstrate: 11523 Style FiberglassThis data represents typical values for the production mate.. |
|||
Thickness | 152 microns | 6.00 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 514B12R006 0.006" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 1.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 2116 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Thickness | >= 152 microns | >= 6.00 mil | Side 2 |
Arlon 51583R020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Thickness | 152 microns | 6.00 mil | Side 2, Layer 2; Arlon SQA-TMS-003 |
Arlon 55148R036 0.036" (0.914 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber This data r.. |
|||
Thickness | 152 microns | 6.00 mil | Liner |
3M 9672 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Thickness | 152 microns | 6.00 mil | Side 2, Layer 1; Arlon SQA-TMS-003 |
Arlon 55578R036 0.036" (0.914 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Appearance:.. |
|||
Thickness | 152 microns | 6.00 mil | side 1; Arlon SQA-TMS-003 |
Arlon 56976B026 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 152 microns | 6.00 mil | side 1; Arlon SQA-TMS-003 |
Arlon 56976R026 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber |
|||
Thickness | 152 microns | 6.00 mil | side 2; Arlon SQA-TMS-003 |
Arlon 56976XA026 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber |
|||
Thickness | 152 microns | 6.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 56986XA028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flame Resistant-flexible heater substrateApp.. |
|||
Thickness | 152 microns | 6.00 mil | Side 1, Uncured Layer; Arlon SQA-TMS-003 |
Arlon R35948R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberThis data re.. |
|||
Thickness | 152 microns | 6.00 mil | Overall; Arlon SQA-TMS-003 |
Arlon R37230R006 0.006" (0.152 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Substrate Design/Construction: Liner: FEP Add-on: Uncured Silicone Rubber Substrate: PTFE Coated Fiberglass This data represents typical values for the production material. The data should not be used to wri.. |
|||
Thickness | 152 microns | 6.00 mil | with adhesive |
3M Scotchcal™ IJ5000 Reflective Graphic Film' 6-mil, enclosed lens, retroflective, flexible films; Pressure-sensitive adhesive; Permanent; Available in white only; Similar daytime and nighttime appearance that retains most of its reflectivity w.. |
|||
Thickness | 152 microns | 6.00 mil | Total |
3M 1115B EMI Shielding Tape 3M EMI Shielding Tapes are well suited for applications requiring reliable point-to-point electrical contact, particularly EMI shielding, grounding and static charge draining.Information provided by.. |
|||
Thickness | 152 microns | 6.00 mil | Tape |
3M 410M Double Coated Paper Tapes 3M™ Double Coated Paper Tapes 401M and 410M utilize a natural rubber adhesive system that offers good to excellent adhesion to many types of surfacesInformation provided by 3M |
|||
Thickness | 152 microns | 6.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 51273R020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave: Polyethylene This data represents typical values for the production materia.. |
|||
Thickness | 152 microns | 6.00 mil | Side 1 |
Arlon 51581R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the.. |
|||
Thickness | 152 microns | 6.00 mil | Side 2 |
Arlon 51581R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the.. |
|||
Thickness | 152 microns | 6.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55276R026 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Uncured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red si.. |
|||
Thickness | 152 microns | 6.00 mil | Layer 1; Arlon SQA-TMS-003 |
Arlon 55279R055 0.055" (1.40 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s.. |
|||
Thickness | 152 microns | 6.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 56866R026 0.028" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil LDPEThis data represents typical values for the production mater.. |
|||
Thickness | 152 microns | 6.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 56986R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flame Resistant-flexible heater substrateApp.. |
|||
Thickness | >= 152 microns | >= 6.00 mil | Side 2 |
Arlon R33979C028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Layer Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in p.. |
|||
Thickness | 152 microns | 6.00 mil | Side 1, Uncured Layer; Arlon SQA-TMS-003 |
Arlon R35928R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: .. |