Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 1270 microns | 50.0 mil | nom |
Mid-Mountain Materials SILTEX® 36 Amorphous Silica Textile Description: SILTEX is a family of high performance textile fabric that is comprised of high purity, high strength amorphous silica fibers, woven into a strong, flexible fabric designed for use wher.. |
|||
Thickness | 1270 microns | 50.0 mil | |
Zircar Ceramics APA-2 Alumina Paper ZIRCAR Alumina Papers are uniform structures made principally of alumina fiber. APA-2 is a flexible un-bonded sheet that contains no organic binder. Applications include thermal insulation in low .. |
|||
Thickness | 1270 microns | 50.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 10322B050 0.050" (1.27 mm) Fully Cured Silicone Rubber with Polyethylene Liner Design/Construction:Liner: Polyethylene Material: Fully Cured Silicone RubberProduct Use: Anti-Static Vacuum BaggingAppearance: Black elastomeric sheetThis data represents typical values for the pro.. |
|||
Thickness | 1270 microns | 50.0 mil | Silicone; Arlon SQA-TMS-003 |
Arlon 32980X050 0.050" Uncured Silicone Rubber on Polyester Film Design/Construction:Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as material.. |
|||
Thickness | 1270 microns | 50.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 51146R050 0.050" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PEThis data represents typical values for the production materi.. |
|||
Thickness | 1270 microns | 50.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon E950-10RXX-M8 0.050" (1.27 mm) Cured Silicone Rubber with PSA liner Description: 1 inch wide, 50 mil thick, Red, Rectangular cross-section, Fully cured silicone interleaved with 0.002” PSA liner. Product is supplied in various roll lengths and the xx in the product.. |
|||
Thickness | 1270 microns | 50.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon LW50125R##-P1 0.050" (1.27 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1.25 inch wide, 50 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll lengt.. |
|||
Thickness | 1270 microns | 50.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon LW50125Rxx-P0 0.050" (1.27 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1.25 inch wide, 50 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Design/Construction: Interleave: Polyethylene Rubber: Cured Self-Fusing Silicone Rubber Cross-Se.. |
|||
Thickness | 1270 microns | 50.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon LW5015Y##-M1 0.050" (1.27 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1.5 inch wide, 50 mil thick, Yellow, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll len.. |
|||
Thickness | 1270 microns | 50.0 mil | Arlon SQA-TMS-003 |
Arlon R35232B050 0.050" Fully Cured, Static Dissipating Silicone Rubber Fully cured, unsupported, static dissipating silicone.Design/Construction:Liner: 3 mil PolyethyleneProduct: Fully Cured Silicone RubberCarrier: N/AThis data represents typical values for the produc.. |
|||
Thickness | >= 1270 microns | >= 50.0 mil | estimated wet film thickness |
Aremco Corr-Paint™ CP2050-XX High Temperature Protective Coating Epoxy-Phenolic, Glass Fiber Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Thickness | >= 1270 microns | >= 50.0 mil | recommended dry film thickness |
Aremco Corr-Paint™ CP2050-XX High Temperature Protective Coating Epoxy-Phenolic, Glass Fiber Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Thickness | >= 1270 microns | >= 50.0 mil | estimated wet film thickness |
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Thickness | >= 1270 microns | >= 50.0 mil | recommended dry film thickness |
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |