Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 102 microns | 4.00 mil | |
Rogers Corporation XT/duroid™ 8100 0.004" Woven Glass Reinforced Thermoplastic Circuit Material XT/duroid™ 8100 woven glass reinforced thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. XT/duroid 81.. |
|||
Thickness | 102 microns | 4.00 mil | |
Premix Thermoplastics PRE-ELEC® ABS 1415 Conductive Thermoplastic Compound PRE-ELEC® ABS 1415 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® ABS.. |
|||
Thickness | 102 microns | 4.00 mil | |
Premix Thermoplastics PRE-ELEC® TPE 1503 Conductive Thermoplastic Compound PRE-ELEC® TPE 1503 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
Thickness | 102 microns | 4.00 mil | Liner |
Dielectric Polymers NT-240APS High Temperature Laminating Adhesive
(discontinued **) Acrylic adhesive with moisture stable PE coated kraft (60#) liner.Features: Plasticizer migration resistantHigh temperature shear propertiesNeutral pHSolvent resistantApplications: Interior automoti.. |
|||
Thickness | 102 microns | 4.00 mil | Facestock |
3M 7743FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Thickness | 102 microns | 4.00 mil | Release Liner |
3M 9420 Splicing Tape 3M™ Splicing Tapes utilize an acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M |
|||
Thickness | 102 microns | 4.00 mil | Side 1, Cured Rubber Layer |
Arlon 55579R043W 0.043" (1.09 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured layer on top of a cured layer on one side This data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Thickness | 102 microns | 4.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55866R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material .. |
|||
Thickness | 102 microns | 4.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 56606R026 0.027" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production materia.. |
|||
Thickness | 102 microns | 4.00 mil | Side 1 |
Arlon 56606R026M 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass with polymer release li.. |
|||
Thickness | 102 microns | 4.00 mil | without adhesive |
3M Controltac™ 3545C Removable Graphic Film with Comply™ Adhesive 4-mil white, opaque, polyolefin film; Chloride-free film; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Air release channels for fast and easy application; Remova.. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-12 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50--120 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-94 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 microns | 4.00 mil | without adhesive |
3M Scotchcal™ IJ8171 Perforated Window Graphic Film Allows a full image to be seen on the outside while allowing viewing through windows from the inside; 4-mil, opaque vinyl film with a high gloss finish; White on the outside facing image side, black.. |
|||
Thickness | 102 microns | 4.00 mil | ASTM D3652 |
3M 4193-EZ Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 4193-EZ is an easy (EZ) unwind polyethylene tape with a very high-tack adhesive system.Information provided by 3M |
|||
Thickness | 102 microns | 4.00 mil | ASTM D3652 |
3M 4H83W Protective Laser Tape 3M™ Protective Laser Tape 4H83 is a clear or white multi-polymer film coated with medium-tack adhesive designed especially to help provide temporary protection of #3 & #4 stainless steel sheets dur.. |
|||
Thickness | 102 microns | 4.00 mil | Prime Coated 2113 Fiberglass, Substrate |
Arlon 47091R012 0.012" (0.305 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data should not be u.. |
|||
Thickness | 102 microns | 4.00 mil | Facestock |
3M 7052W Screen Printable Vinyl Performance Label Products 3M™ Screen Printable Vinyl Performance Label Products are durable, high performance materials that offer good durability and moisture resistance. These vinyl label stocks utilize 3M™ Adhesive P140.. |
|||
Thickness | 102 microns | 4.00 mil | Liner (58# Polycoated kraft) |
3M 8132LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Thickness | 102 microns | 4.00 mil | Liner |
3M 9017FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 9017FL and 9018FL are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. T.. |
|||
Thickness | 102 - 152 microns | 4.00 - 6.00 mil | Side 1 |
Arlon R31861R018 0.018" (0.457 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Thickness | 102 microns | 4.00 mil | Side 1 |
Arlon R33979C028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Layer Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in p.. |
|||
Thickness | 102 microns | 4.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon R38041X012 0.012" (0.305 mm) Uncured Fluorosilicone with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 2116 FiberglassSide 2: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Gray silicone gum.. |
|||
Thickness | 102 microns | 4.00 mil | Liner Material |
3M VHB™ F9460PC Adhesive Transfer Tapes with Adhesive 100MP 3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng.. |
|||
Thickness | 102 microns | 4.00 mil | estimated wet film thickness |
Aremco Corr-Paint™ CP2020 High Temperature Protective Coating Urethane, Aluminum Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Thickness | 102 microns | 4.00 mil | without adhesive |
3M 3635-20b Diffuser Film Control light transmission or achieve special effects for backlit signs; 2 and 4-mil vinyl film; Pressure-sensitive adhesive and Adheres to rigid or flexible substratesInformation provided by 3M |
|||
Thickness | >= 102 microns | >= 4.00 mil | Side 1 |
Arlon 44560R009W 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Appearance Red silicone gum on glass fabricThis data represents typical values for the production material. The data should not be used to write, .. |
|||
Thickness | 102 microns | 4.00 mil | Prime Coated 112 Fiberglass, Substrate |
Arlon 43191R012 0.012" (0.305 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. T.. |
|||
Thickness | 102 microns | 4.00 mil | Average value: 102 microns Grade Count:8 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |