Polymer Property : Cell Length = 0.250 mm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Cell Length 0.250 - 0.600 mm
0.00984 - 0.0236 in
Zotefoams Evazote® EV50 Ethylene Vinyl Acetate Copolymer Foam
Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta..
Cell Length 0.250 - 0.700 mm
0.00984 - 0.0276 in
Zotefoams Plastazote® HD30 High Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Cell Length 0.250 - 0.800 mm
0.00984 - 0.0315 in
Zotefoams Plastazote® LD18SC Low Density Polyethylene Foam, Small Cell
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Cell Length 0.250 - 0.550 mm
0.00984 - 0.0217 in
Zotefoams Plastazote® LD33 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Cell Length 0.250 - 0.600 mm
0.00984 - 0.0236 in
Zotefoams Plastazote® LD33FM Low Density Polyethylene Foam, Flame Retarded
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Cell Length 0.250 - 0.600 mm
0.00984 - 0.0236 in
Zotefoams Plastazote® LD45 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Cell Length 0.250 mm
0.00984 in
Zotefoams ZOTEK® N B50 High Performance Nylon Foam
Zotek® N B50 is a closed cell, cross-linked polyamide-6 foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Cell Length 0.250 - 0.550 mm
0.00984 - 0.0217 in
Zotefoams Plastazote® LD38 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Cell Length 0.250 - 0.600 mm
0.00984 - 0.0236 in
Zotefoams Plastazote® LD45FR Low Density Polyethylene Foam, Flame Retardant
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Cell Length 0.250 mm
0.00984 in
Zotefoams ZOTEK® F 35 PVDF Foam
Zotek® F 35 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o..
Cell Length 0.250 - 0.550 mm
0.00984 - 0.0217 in
Zotefoams Plastazote® LD34 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..