Physical Properties Metric English Comments
Melt Flow 0.300 - 80.0 g/10 min
0.300 - 80.0 g/10 min
Average value: 17.1 g/10 min Grade Count:130
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Melt Flow 1.00 - 80.0 g/10 min
1.00 - 80.0 g/10 min
Average value: 25.0 g/10 min Grade Count:9
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Melt Flow 60.0 - 80.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
60.0 - 80.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBB2672 Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (500000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex
Melt Flow 0.0800 - 80.0 g/10 min
0.0800 - 80.0 g/10 min
Average value: 14.7 g/10 min Grade Count:399
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..
Copyright © lookpolymers.com All Rights Reserved